View Full Version : trailer gate in the making
fastcat
04-04-2007, 11:38 PM
here are some pics of the gate i am making for my trailer. I still have to get the flux dust off of it before paint.
MicroZone
04-04-2007, 11:43 PM
Looks like it will be a medium duty ramp, good job. Welcome to weldingweb!
Will it server double duty as a ramp for mowers?
fastcat
04-05-2007, 12:24 AM
yep, its for my bobcat 42inch ztr. 2x2x1/8 angle iron.
fun4now.
04-06-2007, 01:41 AM
nice job, are you going to cover it in expanded sheet ??
welcome to the show by the way. :)
fastcat
04-14-2007, 07:25 PM
here are the rest if the pics.
fastcat
04-14-2007, 07:28 PM
more pics .......
fun4now.
04-15-2007, 01:19 AM
loots of splatter, but it shore came out nice in the end.:D great job.