PDA

View Full Version : Guide Rollers..


zapster
10-24-2007, 03:50 PM
Yep..
More and more!!!

These are diffrent though..
Most we do have screw on end plates but these are welded..

Same taper-lok set-up as all the rest..
(But I hav'nt done the bushings yet)

Wanted to get them together and rough turned before hand so there will be less "beating" on the shaft afterwards..

Roller..
13490

Head root pass..
13491

13492

Stitch cover pass..
13493

13494

Next!

...zap!

zapster
10-24-2007, 03:57 PM
After cooling down outside it's back in the machine for "end prep"

End Prepped..
13495

Here is the ring for the outside edge..
Blanchard ground to .312..
13496

Nice weld champhers..
13497

Outside root pass..
13498

Cover stitch pass..
13499

These will be machined flat when done..

As we get deeper into it I'll post the end result tomorrow..

I get all the fun jobs..:cool:

...zap!

Bikespot
10-24-2007, 06:06 PM
Nice

Looking good ,

When it gets machined down will there be any of the weld filler left?

zapster
10-24-2007, 06:26 PM
will there be any of the weld filler left?

I doubt it..

They want smooth sides so that's what they get..

...zap!

MoonRise
10-24-2007, 06:37 PM
Ho-hum. Yet another job by zap with consistent and clean TIG welds on some round parts. :laugh:

Good job. Again.

but ripple number 792 looks slightly different from ripples 791 and 793. tsk, tsk, tsk. :jester:

zapster
10-24-2007, 08:31 PM
Ho-hum.


Exactly...:sleeping:

I want to do something square with hills and valleys..:laugh:

...zap!

Rick Moran
10-24-2007, 08:48 PM
Nice work Zap. I think it's great that you do such consistently perfect "boring" jobs. :laugh: :laugh: I wish I were that boring....

spiral-cut-bevel
10-24-2007, 10:08 PM
the stitches look gorgeous...:blush:

Diehard
10-24-2007, 10:25 PM
thats purdy zap, nice work.