i dug it out of the garage today, it is a hobart hi-fr attachment
220 volt
weld current max 500 amp
model 966 specs 4466
ser. no. AATW-2403 var. 2-5
can anyone tell me how to set this up and i need a wiring diagram because therre are a couple of loose wires inside.
David R
01-13-2008, 06:12 PM
Can I see a pic of the front and spec plate?
David
G3farms
01-13-2008, 06:13 PM
more pics (bare with me just learning)
15515
15516
15517
15518
scubaholic
01-15-2008, 10:37 PM
wanna sell it?????????
David R
01-16-2008, 05:37 AM
That is the biggest Hi freq/water cooler I have ever seen!
David
KSellon
01-16-2008, 09:40 AM
G3- I have a manual on this High Freq Arc Stabilizer. Do you have a fax number? The manual is 29 pages.
G3farms
01-16-2008, 05:38 PM
Ksellon..........yes I have a fax number and would love the manual for it. I am glad someone answered on it because I was thinking of scrapping it.
Thanks in advance!!:)
pm sent to you.
Scubaholic......I think I will play with it for the time being and see what I can do with it. If I decide to sell it I will post it here first and then ebay.
G3
pulser
01-16-2008, 06:33 PM
That is the biggest Hi freq/water cooler I have ever seen!
David
No water cooler, just HF arc starter with solenoid valves for gas and water on/off.
G3farms
01-16-2008, 07:10 PM
This has been sitting in the garage for about 7 or 8 years, I had almost forgotten that it was in there. Wife and daughter buried it over in the corner and I aught a glimpse of it the other day.
What kind of power source do I need to hook onto this?
G3
weldersales
01-31-2008, 12:28 PM
Any stick welder will work, but if you want to do aluminum, use an ac/dc welder. weldersales
TozziWelding
01-31-2008, 05:13 PM
It is a primitive form of the Miller HF-251D.