brimy311
10-24-2004, 08:42 PM
I just bought a new powermig 255 about a week and a half ago...
Anyways, seem to be having some problems getting a clean weld out of it.
Say i set the machine at 200 Wire feed and 16 Volts, start welding and then the machine will jump to like 20volts and it will start to Spatt.
Anyone have any problems like this?
Anyways, seem to be having some problems getting a clean weld out of it.
Say i set the machine at 200 Wire feed and 16 Volts, start welding and then the machine will jump to like 20volts and it will start to Spatt.
Anyone have any problems like this?