I was subcontracted some structural work on a hotel renovation at a state park in Alabama. Just thought I would post some pics of what's going on.

This is a shot down the lobby.

18913

and then the front as you would drive up.
18914

A few metal studded walls in the soon to be conference center.
18915

Here's my cubby hole where I stay most of the day. I am adding frame work for the roof mounted A/C units to be set on. Going to be about 25 units added on top. You can see the cross bracking of the frames in the back of the picture.
18916

A shot of the old bobcat from up on the lift.
18917

Hammack_Welding
04-17-2008, 10:38 PM
But atleast the scenery isn't to bad...18918

18919

I'll try to get some better pics of the steel working next day I am onsite, and post a few progress pics as it goes along....:waving:

smithboy
04-17-2008, 10:41 PM
Which state park? They re-did the one up at Guntersville not too long ago...it took years to complete. My wife and I frequent the AL state parks because we are pretty close to several. Cheaha is close also and is one of our favorites. You could be in for a full-time job for a while.

Those last two pictures look like Guntersville! Are they still working on that?!

Hammack_Welding
04-17-2008, 11:34 PM
It's Lake Point In Eufaula, AL on Lake Walter F. George. It's a two year renovation contract, but the bulk of what I am going to do will be done within the next couple weeks. However, I will be in and out until all the welding on the job is finished. .