I was wondering if anyone out there knows where to find info on testing with diesel fuel. We are welding 14 ga stainless on tanks and we test for leaks with diesel fuel. One of our customers is asking for some fancy scientific description of this test. Has anyone ever seen this technique in an article or book anywhere?
Thanks, Andy