View Full Version : Cut 50d
Brooksy
09-17-2008, 05:10 PM
I bought this cut 50 on ebay. It will not cut, all it does is blow air. I get a very tiny little spark when I squeeze the trigger. Ihave tried different distances to start from touching to a quarter inch away. I am getting frustrated with this damn thing. I have sent emails to your help site and all I got was an auto generated email. HELP!
EVERLAST_SUPPORT
09-17-2008, 05:22 PM
I bought this cut 50 on ebay. It will not cut, all it does is blow air. I get a very tiny little spark when I squeeze the trigger. Ihave tried different distances to start from touching to a quarter inch away. I am getting frustrated with this damn thing. I have sent emails to your help site and all I got was an auto generated email. HELP!
Please PM me your phone number or Email address and I will contact you and see what is going on. I have been on the forum here on and off all day and have not received your emails.
I will find out what is going on there once I talk to you. Not sure?
To PM (private message), Click on everlast_support on the left top of this message, then send a private message. Just need an email or phone number and I will get right back to you.
Mike
Brooksy
09-17-2008, 05:29 PM
306 445 7206
brooksy9p1q@sasktel.net
MX727
09-17-2008, 11:15 PM
If his looks like my unit, the little switch has to be in the off position. Found that out today. Mine acted like Brooksy's until I flipped the switch.