I would like to say the welding charts on the inside of my Lincoln Pro MIG 175 are not so great.
I think the person who made it got lazy. They are using the same settings for metals that are .030 different in thickness.
This caused a lot of confusion when trying to get setup to MIG 1/8" steel. I finally noticed what was going on and now my welds are coming together.