PDA

View Full Version : Recent structural work.


admswelding
11-09-2008, 07:44 PM
These are a few pics of a couple of structural jobs i,m in the process of finishing now.One is 12"x4"x3/8" HSS 15' '-6"'Long gusseted with 6"x4" 1/2" 9' long HSS all galvanized because its in a car wash bay.The other is 12"x4" 5/16" vertical HSS with a W10- 49 lbs/ft 18'-9" long on top.With me fluxcore welding on the laddwer.:D

patrickp
11-09-2008, 08:30 PM
good ole galvanized metal. always fun to weld. looks like a single bay car wash? jobs in town like that are always good for free advertising.

farmersamm
11-09-2008, 08:30 PM
Will there be machinery suspended from the clear span, or is the local building code picky about clear spans. Galv. because of moisture from car wash?

Another story above it?

admswelding
11-09-2008, 08:38 PM
Lentil clips hanging down now, i did them today i,ll get some pics of them and post them later.galv yes, lots of moisture i recomended that to the building owner.

welderShane
11-09-2008, 10:03 PM
Looks good so far!!

admswelding
11-16-2008, 07:53 PM
Few more as the job moves forward, also had to add to the lentils thanks to the engineers mistake had only 7-1/2"to hold 11-1/2"concrete arch not gonna work:nono: but i fixed it, just have to paint bare steel that didn,t get galvanized. Carpenters came also as you can see.:waving:

MoonRise
11-17-2008, 12:08 PM
Ahhh "lintel" !!

I couldn't figure out why you were using lentils (a small seed, from a plant in the pea family, there's this diner I go to sometimes that usually has this pretty good lentil soup ... ) as part of a building. :laugh:

Don't forget that you left your magnetic 4-ft level on the angled column. :laugh:

That arched lintel looks nice.

lewray
11-17-2008, 12:21 PM
Looks like some good work there:cool:

mark8310
11-17-2008, 01:28 PM
I notice you signed your work too, Billy ....... Been known to do that once or twice myself

admswelding
11-18-2008, 08:33 PM
I notice you signed your work too, Billy ....... Been known to do that once or twice myself
Lets the local welding co's, that know me or not,know i was there.:laugh:

admswelding
11-19-2008, 05:02 AM
I just reread my first post here those vertical columns are 12"x6" not 4" my bad just to clarify things if anyone actually cares.:dizzy: