So I got my Sync 200 back in june and only have a few hours with it. Too busy with school and stuff. Only thing I built was a downpipe and some charge piping for my civic turbo project.

I recently found a nice 3/4" thick piece of steel at a local yard for $50 (3/4" x 4.5ft x 3.5 ft)
I used some 2.5" round pipe I had lying around for the legs, and braced them with 1" square.

Here are some pics when I first got it, then I finished it up today.

Just waiting on some friends to help me flip it over, then I can wire wheel the top and start welding away!

http://img383.imageshack.us/img383/21/img0540tp2.jpg


http://img262.imageshack.us/img262/6912/img0539ze2.jpg


http://img142.imageshack.us/img142/2111/img0546zk8.jpg


http://img370.imageshack.us/img370/2495/img0549tl8.jpg


http://img206.imageshack.us/img206/7033/img0550eg3.jpg

partagas
12-15-2008, 08:39 PM
I would put cross braces on the legs. That is a big table to risk falling when you dump something heavy on it.

Bob
12-16-2008, 12:17 AM
You should have put the legs and braces back under the table aways so they wouldn't get in the way of clamping things down. I made the same mistake on mine.

m R g S r
12-16-2008, 12:44 AM
I figured the triangles would support the legs enough if the table happens to shift, which I doubt it will because I don't plan on putting that much weight on it.

And with the size of the table, I think I have enough room to clamp around the spaces where there are no legs/support bars....

Mustangous
12-16-2008, 12:50 AM
looks good.. Good deal on the steel! :drinkup: