View Full Version : Need help testing a gas welder
Ag Specialties
03-12-2009, 02:42 PM
Guys i have a guy that thinks his welder isn't working. Wants me to weld with it. He had a guy tell him that it is welding like it is DC- all the time. I checked the lever and the contacts are working. I am going to weld with it in a little bit.
I will let you know
OH by the way
Miller Trail Blazer 301G
lugweld
03-12-2009, 03:43 PM
What gas is he using? DC neg is flux core territory. What are the symptoms? Most likely, it is either a wire feed issue or too slow of a feed rate.
tnjind
03-12-2009, 07:09 PM
I am assuming (i know) that it is stick weld (SMAW).
Ag Specialties
03-12-2009, 08:53 PM
There was nothing wrong with the welder. Guy didn't know how to set up the welder.
Dumb ***