pat.v
08-23-2005, 03:37 PM
As a newbie have enjoyed and learned so much from this forum.Thanks. My question is suggested settings (gas, speed etc) for welding a tubular steel fence using 1x1' rails 1/16 inch thick to 5/8" verticals. Have a Miller 210 and using .023 wire. The bead is so short between the start and end that I can't get a smooth run. Does a speed of 30, setting of 2 and 15 cu ft sound right?