View Full Version : ladder cage
19662
08-18-2009, 08:04 AM
A local industrial facility asked me to give them a quote on fabricating some ladder cages for them. I was wondering if there was a link to what the OSHA specs would be or maybee one of you might already know. Thanks
weldinglifer
08-18-2009, 09:03 AM
CFR 29 will take you to the OSHA Standards
JBFab
08-18-2009, 09:42 AM
OSHA put out this publication which lays it out pretty nicely:
http://www.osha.gov/Publications/osha3124.pdf
I draw quite a few of these ladders, and could send you a print if you would like.
19662
08-18-2009, 10:54 AM
I would greatly appreciate that JBFab thanks. I dont know if i'm gonna get the job, but if I do I'd like to build them to specs, this is a valued customer.