PDA

View Full Version : PowCon 150stp tig welder


david koontz
11-10-2009, 10:43 PM
Any one know anything about these welders? this unit was used as a power supply on a coil splicer my company junked out.worked good for this it is 230 volt ac single phase, dc out put only. does anyone know where you can get a foot control for it? All I have is the unit, have used it with my tig torch but have to try to control off panel. Maybe some one wants it cheap? 100$ located north central tn THANKS TO ALL TNE PEOPLE WJO MAKES THIS FORUM SO GREAT

DesertRider33
11-10-2009, 11:14 PM
I don't know anything about that particular model. I have a PowCon 300SM stick/mig unit that works very well for stick welding. We used to use a few of these at my old job to pulse mig weld aluminum, along with a few other machines. They're great little machines.

Try www.arcproducts.com, the official PowCon service center and experts on all things PowCon. Also try www.ssccontrols.com, makers of foot pedals for just about any machine around.