Here is a quick documentary of a trailing arm build I recently completed for an R1 buggy project I am working on.

Paper templates (old school)
44109

watercut parts finished
44110

Inner components welded:
44111

Overall view:
44112

Fitup for welding
44113

Airwolf
01-10-2010, 07:00 PM
Continued...

couple welds...
44114

and DONE!
44115

DSW
01-10-2010, 07:06 PM
I like the jig. Can you do both sides with the same jig or do you have to rebuild it to do the second side? I'm amazed at how often guy's won't take the time to make a simple jig like this to do a job. Often it's much faster and simpler that trying to work without one.

Nice work.

kenklingerman
01-10-2010, 07:09 PM
excellent!

Airwolf
01-10-2010, 09:26 PM
Yes, both sides can be built with the same jig. Toe is neural , camber is set using shims in the jig on the microstub.

The jig was not only usefull in setting wheelbase, but in welding to help control warpage