the machine runs, the wire feeds but won't burn the wire. this happen once before but started working again. can anybody help?

TBD
01-09-2006, 10:36 AM
what happen may come in handy for someone else and I was lucky to find out the problem. Something told me to check the Voltage coming in my house and I was getting 253 volts. My mig was shutting down. I called DEMCO my Electric CO. and they came out checked to see if I was wright ( I was ) hurried to the substation and turn it down

chopper5
01-09-2006, 05:31 PM
i had a simler thing happen at work the compersure keep bolwing fuses i checked
the in comeing volts not 440 v like it should be 575V i called con ed told them
thay told me thay did not have a problem but an hour later it was back down to