07-17-2010, 02:58 PM
Anyone have trouble with tig aluminum and high heat/humidy?
thanks jon

bassboy1
07-17-2010, 06:23 PM
Yep. Had the problem just today. The helmet lens fogs up, and I can't see jack diddley squat.

makoman1860
07-17-2010, 07:18 PM
Shouldnt be much of an issue since the atmosphere of the weld pool is your shielding gas for the most part. Might be fighting pre-weld oxidation a little more. I have had more issue with humidity in the shielding gas than anything, before installing line dryers. Hmmm unless your in a coastal area where the humidty is a bit "salty"....hmmm. But that should be cured with a good prep as well.