02-18-2006, 01:31 PM
I ordered a Tweco mini mig gun for my welder and tweco says it's a direct replacement for my welder (just lighter duty and I need it for tubing) I received it a couple of days ago but the actual brass or copper male end connection that gets inserted into the welder is missing? Has anyone else had this problem?

JR Beas

fastgmc98
02-19-2006, 07:20 PM
I think it requires an adapter. I can't find one on the tweco website.

fastgmc98
03-05-2006, 09:13 AM
Finally I talked to Tweco and they told me that they don't make an adapter for my welder and the mini mig gun because the drive rolls on the Lincoln Power Mig 255C are angled? Don't understand!!! Anyways sent it back and got another Tweco mig gun the FABMASTER. Very light and compact!