02-22-2006, 10:43 PM
I bought a ln 10 wire feed and i have trouble with burn back and getting a good setting does anyone one have some tips that may help. The number1 thing that gets to me is tacking with it on thin guage steel it stutters and then fires up long enough to ruin the tip or leave pin holes arg I am using .035 solid mig wire on clean steel

etuke
03-14-2006, 08:02 PM
your using gas with it right?

fireblade
03-14-2006, 09:52 PM
yeah 80/20 carbon argon mix

Denni
09-20-2006, 09:14 AM
Try 75/25 argon/co2