assassin_works
08-27-2010, 06:44 PM
what do you think
a but weld weld in a push at 160amp with 7018 dc rods
http://i263.photobucket.com/albums/ii132/urbanswat/PICT0035.jpg
this is abut weld in a pull direction at 160amp with 7018 dc rod
http://i263.photobucket.com/albums/ii132/urbanswat/PICT0033.jpg
this is a T joint weld and it is on a push direction 160amp 7018 dc
http://i263.photobucket.com/albums/ii132/urbanswat/PICT0039.jpg
:blob2:
a but weld weld in a push at 160amp with 7018 dc rods
http://i263.photobucket.com/albums/ii132/urbanswat/PICT0035.jpg
this is abut weld in a pull direction at 160amp with 7018 dc rod
http://i263.photobucket.com/albums/ii132/urbanswat/PICT0033.jpg
this is a T joint weld and it is on a push direction 160amp 7018 dc
http://i263.photobucket.com/albums/ii132/urbanswat/PICT0039.jpg
:blob2: