For starts, one of the first things on my list involves attaching 1/2" stainless rod to 1/4" mild steel plate. I've seen what to use to weld stainless to stainless and mild to mild, but never one to the other. Is that because you can't do it? Or that it just doesn't come up often?
Thanks, Wm

OlPilot
02-19-2004, 03:47 PM
For carbon steel to stainless, I'd recommend 309 stainless rod (AWS E309-15, AWS A5.4-69)

Franz
02-19-2004, 04:48 PM
309 will get the job done. You may want to do a bit of practicing on scrap before you make the critical weld you need thought.