View Full Version : Lincoln V205T on 115v
typerr
06-12-2006, 10:21 AM
I just picked up a used Lincoln V205T Tig Welder and would like to get it going on 115v until I can get the proper 230v outlet installed in my garage. Lincoln says to rewire the cord with a 115v plug but I'm wondering if anyone knows where I can get an adapter to go from the 230v plug to a 115v plug.
Thanks
MAC702
06-12-2006, 12:37 PM
Several online welding shops sell them, but you can make one with parts from HD a lot more simply. Which 230/250V plug does it currently have?
I think the adapter is definitely a lot smarter than rewiring it. That way, you'll always have that capability.
Like the Miller Dynasty/Maxstar series, it'll automatically connect to the different voltage.
Pentawelder
06-12-2006, 12:44 PM
Here's the link to the manual on Lincoln's site
http://content.lincolnelectric.com//pdfs/products/navigator/im/IM728.pdf
Section A4
typerr
06-12-2006, 03:43 PM
Several online welding shops sell them, but you can make one with parts from HD a lot more simply. Which 230/250V plug does it currently have?
I think the adapter is definitely a lot smarter than rewiring it. That way, you'll always have that capability.
Like the Miller Dynasty/Maxstar series, it'll automatically connect to the different voltage.
It has the 6-50 three prong plug. Can you post a link, I'm having a heck of a time finding the adapter.
Thanks
MAC702
06-12-2006, 05:56 PM
It has the 6-50 three prong plug. Can you post a link, I'm having a heck of a time finding the adapter.
Yeah, I'm having trouble finding them, now, too.
If Home Depot or a real electrical house is near, you can make the adaptor for around $20 in parts.
You need a NEMA 6-50R receptacle, preferably one with the box and receptacle all-in-one; any length of 12/3 SO cord; and a NEMA 5-15P plug.
Now, the NEMA 6-50 is designed to accept a #10 minimum, so I just double over the #12 under the terminal screws. This is much better than trying to get that #10 cord to work with a NEMA 5-15 plug.
typerr
06-12-2006, 06:33 PM
Yes, I'll head to HD tonight.
What do you do about the fact that the 6-50 has two hot leads while the 5-15 has one hot and one neutral?
Thanks
MAC702
06-12-2006, 06:58 PM
The welding machine knows how to switch them on the inside. Connect one "hot" to the "neutral" prong of the 120V plug.