View Full Version : Samples of welding TIG.
Good day to all!
I decided to post pictures of the samples of welding.
1. I'm at work.
2. I'm at work.
3. Copper + steel.
4. Steel + steel 3 mm.
5. Steel + steel 3 mm.
1. Copper + Copper
2. Steel + steel 10 mm
3. Steel + steel 10 mm
4.Steel 10 mm
5. Steel 10 mm
1. Steel + steel 3 mm
2. Steel + steel 3 mm
3. T-joint steel 3 mm
4. Pipe diameter 70 mm
5. Pipe diameter 70 mm
1. Steel 0.5 mm
2. Steel 0.5 mm T-bar
3. Steel 0.5 mm T-bar
4. Profile welding
5. Profile welding
Ready to hear your views on our samples. TIG welding work was performed.
zapster
08-11-2011, 04:36 PM
I hope you are ready..
Work on it and get a better camera.
...zap!