PDA

View Full Version : stainless but weld no filler 14 gauge at 80 amps



Ron Padilla
12-06-2011, 03:43 AM
havent been doing much lately so I grabbed a few coupons and melted them together next I need to get may hands on 16 guage tube. hit me what you think. this is 14 gauge done at 80 amps with no filler check both sides.

tnjind
12-06-2011, 06:34 AM
I see you have been to the Miller site.......

David R
12-06-2011, 07:32 AM
Try a lap using some of the base as filler.

Looks pretty good, needs less heat.

Do it again!

David

Ron Padilla
12-06-2011, 01:37 PM
i have more so going to do the laps, i have been to the miller site along rig weider, and a few others

tnjind
12-10-2011, 10:43 AM
i have more so going to do the laps, i have been to the miller site along rig weider, and a few others

I see the tig for dummies book from Miller, I have one too.

Ron Padilla
12-11-2011, 05:23 PM
the one in the photo is daily spanish for dummies, the tig book is out in the garage, I read anything I can get my hands on

Mikel_24
12-11-2011, 05:50 PM
Never used a tig torch but I could help you out with your Spanish... LOL.

That fusion weld looks good to me. As soon as I get a bottle of pure argon I will give TIG a try (already have everything else).

Mikel

Ron Padilla
12-12-2011, 04:57 PM
Thanks for the offer to help with spanish, if you wanted to you could pick up 3 one way tickets to your location I could help you tig and you could help me with spanish just let me know when to get ready.