PDA

View Full Version : Tig


lil john
09-24-2006, 04:47 PM
How can I put a TIG on a Miller Bobcat 225G?

slamdvw
09-25-2006, 04:06 AM
I believe Miller has a kit that has the necessary parts... If not... a connector block, TIG torch ( with accociated hardware: cup, collet and body, tungsten ) gas bottle and regulator or flow meter. Work clamp Positive, torch - Negative.

Hopefully I answered your question.

Robert

Engloid
09-25-2006, 11:11 PM
I have exactly what you need. I used to get asked this so much that I did a detailed writeup about it, and and another guy asked to host it and keep it online.

http://www.az-zbum.com/welder.upgrade.shtml

lil john
09-26-2006, 10:55 PM
Ok how do I control the gas to the torch.

elvergon
09-26-2006, 10:57 PM
Regulator.

lil john
09-26-2006, 11:04 PM
So is the gas always on even when not welding.

Sober_Pollock
09-26-2006, 11:18 PM
Get A torch with a valve on it.