01-25-2012, 09:41 PM
Will it work on 208? Plate says 240/480.

Not my machine, but I knew where to find you.

David

jimcolt
01-26-2012, 01:06 PM
It may work....but not to its full potential. This is a transformer/chopper power supply design which is more voltage sensitive as compared to the newer air plasma technology that uses inverter power supplies with internal voltage boost circuitry.

The symptoms of low voltage on this unit:

1. Misfiring of the torch..or won't fire at all.
2. Diminished output power. Slower cut speeds, more dross, less thickness capacity.


Jim Colt



Will it work on 208? Plate says 240/480.

Not my machine, but I knew where to find you.

David

David R
02-13-2012, 06:53 PM
Thank You :)