Brad-Man
03-16-2004, 02:55 PM
I took welding classes, but they had flowmeters, the Smith's (looks like single stage regulator/guage) sits around 30 lph.
I have loosened the locknut and backed off the screw, but it doesn't go lower.
The manual is sadly lacking in instructions on adjusting w/the supplied guage.
Any tricks that I should know?
Will this setup work for C25 or should I get another guage/flowmeter?
TIA,
Brad