PDA

View Full Version : multipasses


Amalgam
03-24-2004, 07:39 PM
Hey you guys,
I am a big boy now, so I will adventure into the multi-pass welding. Can somebody explain to me the process.
Thank you
Alfredo

Franz
03-24-2004, 10:52 PM
Alfredo, since yer a big boy, you get homework.
Scroll down this site till you get to multilayered welding, and you'll find some good information, and save me a lot of typing.
http://155.217.58.58/cgi-bin/atdl.dll/tc/9-237/Ch10.htm#s2

Amalgam
03-26-2004, 12:53 PM
Thank you Franz every thing I needed to know and more.