MAC702
03-30-2004, 12:02 PM
Okay, here's your chance to do my job!! woo-hoo!
Seriously, I am putting together a chapter for a new manual my office is putting together for inspectors. I am writing the welding chapter.
It will be used for inspectors who may have to substitute a day or so on a job outside of their specialty. For instance, I would take along the chapter on earthwork when I substitute on a highway job.
My chapter will be used by the other inspectors who may have little to no knowledge of welding but there might be SOME welding done on their job. They'll want to know the basics of what to look for.
Give me your thoughts on what topics I should include.
Just off the top of my head, a big section will be on all the different ways you need to be safe while performing various welding procedures.
I'll include a section on what things an inspector needs to record, such as process, polarity, amperage/voltage settings, electrode/wire type and size, WFS.
If using stick electrodes, how were they stored? Was the weldment beveled? Size/shape of weldments?
What would YOU include? And what specifics do you want to make sure _I_ include?
Seriously, I am putting together a chapter for a new manual my office is putting together for inspectors. I am writing the welding chapter.
It will be used for inspectors who may have to substitute a day or so on a job outside of their specialty. For instance, I would take along the chapter on earthwork when I substitute on a highway job.
My chapter will be used by the other inspectors who may have little to no knowledge of welding but there might be SOME welding done on their job. They'll want to know the basics of what to look for.
Give me your thoughts on what topics I should include.
Just off the top of my head, a big section will be on all the different ways you need to be safe while performing various welding procedures.
I'll include a section on what things an inspector needs to record, such as process, polarity, amperage/voltage settings, electrode/wire type and size, WFS.
If using stick electrodes, how were they stored? Was the weldment beveled? Size/shape of weldments?
What would YOU include? And what specifics do you want to make sure _I_ include?