    Bought an enco 12" shear

    So i was told this will cut up to 1/8 plate. Well with the handle it is nearly impossible unless you put all you weight on it. So I took the handle off and put it in my press. Walla it now cuts 3/16 plate. And it was only 90 bucks free shipping
    Attached Images Attached Images  
    Hypertherm Powermax45
    Miller auto 140 mig
    Miller Econotig Watercooled
    with wp24w Torch
    Lincoln Power255XT
    New(Lincoln V205 ac/dc)
    Miller Elite Helmet

  2. #2
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,039

    Re: Bought an enco 12" shear

    I'm missing something here. Is the press pin pushing on the top beam of the shear or on the knife and the ram is just retracted?

    Isn't that the handle extending up thru the upper press beam?
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save 2nd Base!

  3. #3
    Join Date
    Feb 2012
    Location
    Illinois
    Posts
    39

    Re: Bought an enco 12" shear

    Quote Originally Posted by duaneb55 View Post
    I'm missing something here. Is the press pin pushing on the top beam of the shear or on the knife and the ram is just retracted?

    Isn't that the handle extending up thru the upper press beam?
    I have a 1/2 thick by 4" long piece of metal pushing on the blade (not in pic). That is just the stub were the handle attaches. I might modify and install a ram on the unit itself. I have to wait and see how much I use to determine if it is worth installing.
    Hypertherm Powermax45
    Miller auto 140 mig
    Miller Econotig Watercooled
    with wp24w Torch
    Lincoln Power255XT
    New(Lincoln V205 ac/dc)
    Miller Elite Helmet

  4. #4
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,039

    Re: Bought an enco 12" shear

    Thanks for the clarification. Makes sense now.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save 2nd Base!

  5. #5
    Join Date
    Feb 2012
    Location
    Illinois
    Posts
    39

    Re: Bought an enco 12" shear

    Do you see any harm in this. I was going to let time tell,but if anyone knows were a flaw is please yell at me. The gauge only reads about 3.5 tons to shear the 3/16 plate
    Hypertherm Powermax45
    Miller auto 140 mig
    Miller Econotig Watercooled
    with wp24w Torch
    Lincoln Power255XT
    New(Lincoln V205 ac/dc)
    Miller Elite Helmet

  6. #6
    Join Date
    Mar 2009
    Location
    upland, ca
    Posts
    1,102

    Re: Bought an enco 12" shear

    I have the same shear. It works well if you upgrade the handle, clamp the shear and the piece you're cutting down real secure. I find that when when I shear, if I pull the handle in a quick and smooth fashion the distortion is less.

    I think it would be difficult to secure the work piece you're cutting... but if you're cutting narrow or round bars, this set up might help.

  7. #7
    Join Date
    Apr 2012
    Location
    Sarasota
    Posts
    324

    Re: Bought an enco 12" shear

    How long can you cut with this? Never seen a shear like this in action.
    Hobart EZ-Tig newbie.

  8. #8
    Join Date
    Mar 2009
    Location
    upland, ca
    Posts
    1,102

    Re: Bought an enco 12" shear

    biggest cut I ever made on that shear was 1/8" thick plate, the cut was probably about 10 inches. I'm over 200lbs, so I just jump and hand onto the handle, hang on for dear life and let gravity does its work.

  9. #9
    Join Date
    Dec 2011
    Location
    Milford NY
    Posts
    481

    Re: Bought an enco 12" shear

    Where did you purchase the shear?

  10. #10
    Join Date
    Dec 2011
    Location
    Milford NY
    Posts
    481

    Re: Bought an enco 12" shear

    Never mind i had a brain fart, but i did buy one

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement