    Aluminum Penetration

    The welds look good but break very easily. Is it normal or just not enough penetration? They split directly down the center.

  2. #2
    Join Date
    Jan 2004
    Location
    Central PRK
    Posts
    228
    Hmmmn.......I have never seen this. I use 4043 rod. The main problem I have is getting the two pieces to flow together. I seem to end up with too large a bead.