A friend gave me some rod to try and I am quite impressed with it . It is made by Rockmount and it's called Tartan AAA rod. It runs much like 6013 with a little better penetration and has 86,000 PSI tensile. It doesn't need to be kept dry. I did searches for this rod and didn't find much info on it. I didn't see it mentioned on this forum anywhere.
Anyone on here have any experience with it?