    Quote Originally Posted by gxbxc View Post
    Phill did you get a new welding truck and not tell use ??
    Haha, no, I still have the same truck (for now at least)

    Sent from my SM-J327T using Tapatalk

  2. #8652
    Join Date
    Oct 2016
    Location
    Durham, NC
    Posts
    583

    Re: Show us what you welded today!

    Spool gun work on the ladder cover. These are the latches. They will prevent the slop that a traditional latch would allow. There are two.

    I went back and closed that corner too.




    It's a job-shop life.

  3. #8653
    Join Date
    Jan 2014
    Location
    Hallieford, VA
    Posts
    2,695

    Re: Show us what you welded today!

    Welcome back from vacation Dot.
    Jerry
    30+ yrs Army Infantry & Field Artillery, 24 yrs ago

    Miller 350LX Tig Runner
    TA 210, spool gun
    Lincoln 250/250 IdealArc
    ESAB PCM 500i Plasma
    Kazoo 30" vert BS
    Kazoo 9x16 horiz BS
    Clausing 12x24 lathe
    20T Air Press

  4. #8654
    Join Date
    Oct 2016
    Location
    Durham, NC
    Posts
    583

    Re: Show us what you welded today!

    Quote Originally Posted by storeman View Post
    Welcome back from vacation Dot.
    Jerry
    Thanks! It was fun, I got to see some unexpected old friends, made some new ones. I really struggled getting back to work, even though it was welding.

  5. #8655
    Join Date
    Jul 2017
    Posts
    103

    Re: Show us what you welded today!

    Do some aluminium mig weld

  6. #8656
    Join Date
    Jan 2012
    Location
    West Rutland, Vermont
    Posts
    132

    Re: Show us what you welded today!

    Name:  001.jpg
Views: 727
Size:  88.2 KBName:  002.jpg
Views: 722
Size:  85.6 KBName:  003.jpg
Views: 725
Size:  85.0 KBName:  004.jpg
Views: 729
Size:  95.4 KBName:  005.jpg
Views: 725
Size:  81.6 KB

  7. #8657
    Join Date
    Sep 2016
    Location
    Near Traverse City, Mi.
    Posts
    199

    Re: Show us what you welded today!

    @6Boys What is that? Kinda looks like a chiminea on a table top but there is a hole in the bottom of it and the chimney is welded shut. Maybe a big swinging candelabra?
    Miller Dynasty 280 DX, Lincoln 210 MP

  8. #8658
    Join Date
    Aug 2016
    Location
    Sutherlin Oregon
    Posts
    200

    Re: Show us what you welded today!

    Finished this mast today

    Sent from my SM-G920V using Tapatalk

  9. #8659
    Join Date
    Nov 2014
    Posts
    6,201

    Re: Show us what you welded today!

    Looking good Mr consistent. What size cup do U like to use ? And rod?

  10. #8660
    Join Date
    Aug 2017
    Posts
    45

    Re: Show us what you welded today!

    That is truly beautiful - Id love to have that on my boat!

  11. #8661
    Join Date
    Aug 2016
    Location
    Sutherlin Oregon
    Posts
    200

    Re: Show us what you welded today!

    Quote Originally Posted by motolife313 View Post
    Looking good Mr consistent. What size cup do U like to use ? And rod?
    Thanks bud. I like a #7 cup unless I'm in a tight spot then I'll switch to a #5. I usually use a 3/32 5356.

    Sent from my SM-G920V using Tapatalk

  12. #8662
    Join Date
    Nov 2014
    Posts
    6,201

    Re: Show us what you welded today!

    I need to get a long cup there great of tight spots.

  13. #8663
    Join Date
    Oct 2016
    Location
    Durham, NC
    Posts
    583

    Re: Show us what you welded today!

    One of these days 5th street will learn to weld. Sheesh.


    It's a job-shop life.

  14. #8664
    Join Date
    Oct 2015
    Location
    PNW
    Posts
    325

    Re: Show us what you welded today!

    making progress on my biggest project since going out on my own. thought i was going to pulse mig the whole thing but i was wrong. so far its tig on the butt joints and pulse mig on the fillets. i've also finally dialed in my passivating and elctropolishing procedure. its a 10,000 gal 10g stainless tank for a small islands water department. i'm confident in the build now but transportation is the next issue. the state park boat launch has threatened the landing craft operator with legal action if we use their launch. my shop is only a couple hundred yards from the boat launch but now its plan b, c, or maybe z night ops haha. no matter, it will get there and its been a fun build.

    Name:  IMG_20170823_191846.jpg
Views: 621
Size:  109.9 KB
    Name:  IMG_20170823_185733.jpg
Views: 618
Size:  84.7 KB
    Name:  IMG_20170817_200053.jpg
Views: 1351
Size:  70.3 KB
    Name:  IMG_20170817_150244.jpg
Views: 623
Size:  72.2 KB
    Name:  IMG_20170816_160341.jpg
Views: 623
Size:  85.0 KB
    a shop full of welders and equipment

    general contractor specializing in unique problem solving
    commercial industrial and custom residential

  15. #8665
    Join Date
    Apr 2010
    Posts
    2,189

    Re: Show us what you welded today!


    6Boys


    Quote Originally Posted by 6Boys View Post
    Name:  002.jpg
Views: 722
Size:  85.6 KB

    This may be: the most purposeful / poorly over welded / weldment, ever posted . . .

    What is its function . . . ?


    Opus



    ps - is the lifting-eye heavy enough - considering the girth of the knee-band . . . ?

  16. #8666
    Join Date
    Oct 2015
    Location
    PNW
    Posts
    325

    Re: Show us what you welded today!

    and not today but last week, the biggest of the big rigs i've been called in to do a little work on. love them when they are brand new and clean!
    Name:  IMG_20170823_064830.jpg
Views: 617
Size:  104.4 KB

    forgive me. this was the week before that, and only kinda metal related. had to make a one piece stainless door pan for a panoramic door i installed, 18' wide. its not all metal work for me! and who cares to see the boring door pan?! i dont think i'll ever fork out the dough for a door like this but i can appreciate why others would.
    Name:  IMG_20170731_171723.jpg
Views: 625
Size:  72.1 KB
    Name:  IMG_20170731_171434.jpg
Views: 628
Size:  79.3 KB

    promise i'm done, same week as the door. actually on the other side of the lake from the panoramic door, a fire place door. the other work i did there is blah. unique, simple and clean was the customers design request. they seemed happy with it.
    Name:  IMG_20170609_125347.jpg
Views: 628
Size:  125.2 KB
    Last edited by tracymobilecnc; 09-14-2017 at 02:58 AM.
    a shop full of welders and equipment

    general contractor specializing in unique problem solving
    commercial industrial and custom residential

  17. #8667
    Join Date
    Jul 2017
    Posts
    103

    Re: Show us what you welded today!

    625 P

  18. #8668
    Join Date
    Oct 2010
    Location
    Edmonton, AB, CA
    Posts
    264

    Re: Show us what you welded today!

    Quote Originally Posted by 5th Street Fab View Post
    Thanks bud. I like a #7 cup unless I'm in a tight spot then I'll switch to a #5. I usually use a 3/32 5356.

    Sent from my SM-G920V using Tapatalk
    I don't even have to look to see who's post it is. I just recognize your welds right away.
    Very nice.
    You get what you put in and people get what they deserve...

  19. #8669
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    1,700

    Re: Show us what you welded today!

    Quote Originally Posted by tracymobilecnc View Post
    making progress on my biggest project since going out on my own. thought i was going to pulse mig the whole thing but i was wrong. so far its tig on the butt joints and pulse mig on the fillets. i've also finally dialed in my passivating and elctropolishing procedure. its a 10,000 gal 10g stainless tank for a small islands water department. i'm confident in the build now but transportation is the next issue. the state park boat launch has threatened the landing craft operator with legal action if we use their launch. my shop is only a couple hundred yards from the boat launch but now its plan b, c, or maybe z night ops haha. no matter, it will get there and its been a fun build.

    Name:  IMG_20170823_191846.jpg
Views: 621
Size:  109.9 KB
    Name:  IMG_20170823_185733.jpg
Views: 618
Size:  84.7 KB
    Name:  IMG_20170817_200053.jpg
Views: 1351
Size:  70.3 KB
    Name:  IMG_20170817_150244.jpg
Views: 623
Size:  72.2 KB
    Name:  IMG_20170816_160341.jpg
Views: 623
Size:  85.0 KB
    What on earth do they have against you using the boat launch? Nighttime is nice for things like that

    Sent from my SM-J327T using Tapatalk

  20. #8670
    Join Date
    Jan 2012
    Location
    West Rutland, Vermont
    Posts
    132

    Re: Show us what you welded today!

    HTML Code:
    This may be: the most purposeful / poorly over welded / weldment, ever posted . . .
    
    What is its function . . . ?
    
    
     Opus
    Opus,
    I knew you'd say something like that!
    It is a chamber to safely disassemble scrap air brake cannisters.
    Not my design.
    It weighs about 150lbs so I have no doubt the lifting eye will be just fine.

  21. #8671
    Join Date
    Jun 2013
    Location
    BIG SKY COUNTRY
    Posts
    684

    Re: Show us what you welded today!

    Quote Originally Posted by tracymobilecnc View Post
    .. its a 10,000 gal 10g stainless tank for a small islands water department. .
    Name:  IMG_20170823_191846.jpg
Views: 621
Size:  109.9 KB
    Is the base welded on, or something else? Assuming just flat stainless?

    Interesting project.
    Hobbyist - At what point is a "hobby" out-of-control?

  22. #8672
    Join Date
    Nov 2012
    Location
    new york city
    Posts
    6,066

    Re: Show us what you welded today!

    Quote Originally Posted by MetalMan23 View Post
    What on earth do they have against you using the boat launch? Nighttime is nice for things like that

    Sent from my SM-J327T using Tapatalk
    nice work on the stainless tank. the parkies won't let you use their launch? no problem- weld a couple clips with holes,attach some cable and tow the tank to where you need to go. if it'll float that is
    Last edited by docwelder; 09-14-2017 at 07:21 PM.
    i.u.o.e. # 15
    queens, ny and sunny fla

  23. #8673
    Join Date
    Jan 2010
    Location
    Northwest Missouri
    Posts
    1,088

    Re: Show us what you welded today!

    Quote Originally Posted by MetalMan23 View Post
    What on earth do they have against you using the boat launch? Nighttime is nice for things like that
    No Boat ramp. NO problem.


    Name:  IMG_0121.jpg
Views: 475
Size:  62.3 KB
    Roger
    Old, Tired, and GRUMPY

    Salesman will call, Batteries not included, Assembly is required, and FREE ADVICE IS WORTH EXACTLY WHAT YOU PAY FOR IT!

    Dial Arc 250HF
    Thunderbolt 225 AC/DC

    Assorted A/O torches

  24. #8674
    Join Date
    Jan 2014
    Location
    Hallieford, VA
    Posts
    2,695

    Re: Show us what you welded today!

    Many years ago the Army had a similar helicopter we called the CH-54 Sky-Crane or Flying Crane. Could lift heavy artillery, other helicopters or armored personnel carriers and had a "people Pod" that snapped into the middle to transport a whole bunch of troops.
    Jerry

    https://en.wikipedia.org/wiki/Sikorsky_CH-54_Tarhe
    30+ yrs Army Infantry & Field Artillery, 24 yrs ago

    Miller 350LX Tig Runner
    TA 210, spool gun
    Lincoln 250/250 IdealArc
    ESAB PCM 500i Plasma
    Kazoo 30" vert BS
    Kazoo 9x16 horiz BS
    Clausing 12x24 lathe
    20T Air Press

  25. #8675
    Join Date
    Feb 2016
    Location
    Myrtle Beach
    Posts
    239

    Re: Show us what you welded today!

    Got some more work done on the trailer I'm building. It will carry two fuel tanks and hose reels, batteries for pumps etc. To fuel our jet boats.

    Name:  IMG_1640.jpg
Views: 390
Size:  137.5 KBName:  IMG_1641.jpg
Views: 390
Size:  178.5 KBName:  IMG_1643.jpg
Views: 387
Size:  96.7 KBName:  IMG_1638.jpg
Views: 394
Size:  120.5 KBName:  IMG_1639.jpg
Views: 394
Size:  132.8 KB
    Lincoln 350MP
    Millermatic 350P
    Syncrowave 250
    1969 SA200

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement