    Re: External Tig Gas Solenoid - TA211i

    Damn that came out better than I thought. Any room to mount that inside the welder?
    Great work.
    Torchmate 2x2 CNC with Flashcut CNC controls
    Hypertherm Powermax45
    2015 AHP Tig
    Razorweld 195 Mig
    Razorweld 200ac/dc Tig
    ViperMig 180
    Razorweld, SSC Foot Pedal & MK Products & Atlas Positioner Dealer

  2. #27
    Join Date
    Oct 2013
    Location
    NOVA
    Posts
    328

    Re: External Tig Gas Solenoid - TA211i

    Thanks.

    There may be room but I dont think I am gonna even look at it until the warranty is up. Just not worth it when any time I take it off the cart to weld I am doing stick.

    Sent from my SPH-L900 using Tapatalk
    Multimatic 200
    Spoolmatic 100
    Ramco Horizontal Band
    Haberle S225 9" cold saw
    MM 300
    Spoolmate 30A w/ WC-24
    TB 302G
    Dynasty 280 DX Tigrunner

  3. #28

    Re: External Tig Gas Solenoid - TA211i

    The lack of a TIG gas soleniod and being made in China is what made me go with a Multimatic 200.

  4. #29
    Join Date
    Oct 2013
    Location
    NOVA
    Posts
    328

    Re: External Tig Gas Solenoid - TA211i

    Took a look at the switches. The one in the torch is a switch in a circuit board. No ratings listed on it, but the spacings between uninsulated conductors meet UL requirements for 120VAC in industrial controls at least. It is momentary which means my solenoid will on work in 2T mode. If this were an issue to me, I could simply add in an alternating state relay to the mix and make it handle the 4T functions. Not hard, but I dont see the need for my uses.

    As for the TA foot pedal, it is a 250VAC; 15A / 1/2HP rated switch. I think it can handle the 100mA just fine. I designed the controls around using the foot pedal.

    As for the Multimatic 200, I could not justify another 1K for a tig solenoid and a little more portability. Especially when it brings a much lower duty cycle along with it. Dont get me wrong, I think the Multimatic 200 is awesome and would love to have one. It is just not practical at all with my current needs and budget.
    Multimatic 200
    Spoolmatic 100
    Ramco Horizontal Band
    Haberle S225 9" cold saw
    MM 300
    Spoolmate 30A w/ WC-24
    TB 302G
    Dynasty 280 DX Tigrunner

  5. #30
    Join Date
    Dec 2011
    Posts
    952

    Re: External Tig Gas Solenoid - TA211i

    I did a little different setup. I used a 120 VAC gas solenoid and a foot pedal. I don't like messing with the factory wiring in the welder. I use this welder (Thermal Arc 181I) with a finger switch only. With the pedal pre-flow and post-flow are what ever I want. All told I have about $40 in this!






  6. #31
    Join Date
    Apr 2016
    Location
    CA
    Posts
    3,662

    Re: External Tig Gas Solenoid - TA211i

    Nice how do you like it so far?
    '65 Lincoln Idealarc 250 AC/DC
    L-tec PCM-VPi 40A plasma
    ESAB REBEL EMP 215ic
    ESAB Mig Master 250
    Victor Performer O/A

  7. #32
    Join Date
    Dec 2011
    Posts
    952

    Re: External Tig Gas Solenoid - TA211i

    N2......works well......you cam use this with a tig pedal.....but you need to use both feet.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement