tig welding CUNI 6-g
RSS | Subscribe | Contact Us | Advertise | About Us
Results 1 to 2 of 2
  1. #1
    Join Date
    Dec 2009
    Posts
    31

    tig welding CUNI 6-g

    i need some advice concerning a possible test on the above, i can tig weld good but i never ran CUNI what is the standard root opening, also is there any color characteristic i should look for. i will be checking amps on scrap first.

  2. #2
    Join Date
    Nov 2005
    Location
    Santa Fe, NM
    Posts
    1,706

    Re: tig welding CUNI 6-g

    You'll probably want to provide more detailed information on the pipe size and schedule in order to get any meaningful feed back on this.