    Re: Blacksmithing tools

    Well crap... my post got caught in another Penton mini-crash. Woke up to another 3" of snow this morning but I have been back to creating tools out of junk. I had a 24" x 1 1/4" bolt with a square head in my forging pile to work with while I await better weather for the annealing fire for the deep tiller shank tools. We all keep our anvil edges rounded so we don't mark projects, but what if you needed a square edge for a change? The heal of my RR anvil is kept sharp for that reason, but maybe a Hardy tool would be better for a small project. This is another one that should probably be annealed as the bolt head is already chipped and seems a little on the brittle side.
    Attached Images Attached Images     
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A

    Les

  2. #152
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    1,747

    Re: Blacksmithing tools

    Haven't done much with the new toys yet... the grinder is a beast, but I have to get some coolant for the bandsaw before I tackle any big chunks of metal.
    Attached Images Attached Images   
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A

    Les

  3. #153
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    504

    Re: Blacksmithing tools

    Quote Originally Posted by whtbaron View Post
    Haven't done much with the new toys yet... the grinder is a beast, but I have to get some coolant for the bandsaw before I tackle any big chunks of metal.
    I got tired of the mess my coolant system made on my bandsaw. I removed the tank/pump and plumbing and it sits on my shelf now.

    I get great results with quality blades (Starrett atm) and a dry lube stick.

    ​Terry

    **FORNEY**
    180
    230
    **THERMAL ARC**
    210 Fabricator
    181i
    **LINCOLN**
    Idealarc 250/250
    SA 200 (2)
    Ranger 305G LN-25 Pro
    **MILLER**
    Spectrum 625
    Maxstar 150STL
    Syncrowave 351
    XMT 350 cc/cv
    MM 350P

  4. #154
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    1,747

    Re: Blacksmithing tools

    I was looking at the Matrix 2 bi-metal blades at Princess Auto for $60... know if they are any good? Where did you get the dry lube stick? I've never heard of that. It doesn't look like the previous owner used wet lube much either, but I'd guess it's still got the original blade from 2006. The grinder was still in the original shrink wrap packaging and had been on the shelf since 2008. I don't think he's been too active the last 10 yrs. The design of your saw looks VERY similar to the King. This one is set at the 2nd lowest speed... should I go slower with the dry lube?
    Last edited by whtbaron; 04-12-2018 at 08:10 PM.
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A

    Les

  5. #155
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    504

    Blacksmithing tools

    whtbaron:

    I was unable to provide a link but here’s a screenshot of what I use. I bought it from a jobber locally. I would run the saw at normal recommended blade speed with the dry lube. Someone else may have better insight.



    I’m using a Princess Auto blade atm. I’m actually pleased with it. I bought two on sale a couple of years ago so I there’s no guarantee their current inventory is okay or not.

    Hope you’re enjoying your snow. Nice here today.

    Last edited by Lis2323; 04-12-2018 at 08:18 PM.
    ​Terry

    **FORNEY**
    180
    230
    **THERMAL ARC**
    210 Fabricator
    181i
    **LINCOLN**
    Idealarc 250/250
    SA 200 (2)
    Ranger 305G LN-25 Pro
    **MILLER**
    Spectrum 625
    Maxstar 150STL
    Syncrowave 351
    XMT 350 cc/cv
    MM 350P

  6. #156
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    1,747

    Re: Blacksmithing tools

    Thanks for the info... I'll check out the availability of that lube stick locally. So you just pack your snow away with that roller?
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A

    Les

  7. #157
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    504

    Re: Blacksmithing tools

    Yup. Getting old. Easier than shovelling......
    ​Terry

    **FORNEY**
    180
    230
    **THERMAL ARC**
    210 Fabricator
    181i
    **LINCOLN**
    Idealarc 250/250
    SA 200 (2)
    Ranger 305G LN-25 Pro
    **MILLER**
    Spectrum 625
    Maxstar 150STL
    Syncrowave 351
    XMT 350 cc/cv
    MM 350P

  8. #158
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    1,747

    Re: Blacksmithing tools

    So now I'm thinking a spring loaded tube on each side of the blade (something like a brush holder on an electric motor) to hold 2 of those lube sticks in place.... making more work for myself really is an illness... the brush holder should probably be threaded to keep it rotating as the blade wears it down...
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A

    Les

  9. #159
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    504

    Blacksmithing tools

    Good idea but the blade doesn't need a continuous application of the dry stick lube. I just push the tube (cardboard sleeve and all) into the running blade somewhere around once every minute or two of cutting depending on thickness of material.

    I've only used two thirds of a tube in 3 or 4 years. Mind you being retired I don't do an awful lot of cutting. I'm sure in a production environment the flood coolant system would be more efficient.

    I use the same lube stick on my power hacksaw and vertical cutting bandsaw. On my mag drill I usually use the on board coolant system but will sometimes use the dry stick if I don't want a mess.
    Last edited by Lis2323; 04-13-2018 at 11:27 AM.
    ​Terry

    **FORNEY**
    180
    230
    **THERMAL ARC**
    210 Fabricator
    181i
    **LINCOLN**
    Idealarc 250/250
    SA 200 (2)
    Ranger 305G LN-25 Pro
    **MILLER**
    Spectrum 625
    Maxstar 150STL
    Syncrowave 351
    XMT 350 cc/cv
    MM 350P

  10. #160
    Join Date
    Sep 2013
    Posts
    129

    Re: Blacksmithing tools

    Just found out that a water quench is very good for hardening a chipping hammer. Or, good for the crappy chipping hammer I bought at Tractor Supply.

    However, it's not good for a tire iron.

    Both came out very very hard, harder even than the hammer I used to drive them. But the tire iron punch was exceptionally brittle and cracked on me.

  11. #161
    Join Date
    Dec 2015
    Posts
    542

    Re: Blacksmithing tools

    not good for your chipping hammer either, you don't want it "chipping" itself, Wait till the missus goes out and stick it in the kitchen oven on high for an hour or so. Temper it down a bit.

  12. #162
    Join Date
    Sep 2013
    Posts
    129

    Re: Blacksmithing tools

    Quote Originally Posted by jackdawg View Post
    not good for your chipping hammer either....
    No worries, the struck end has been drawn down a bit to soften it. The working end was left at full hardness, but it's meant to work on hot steel and will likely get the hardness drawn down very quickly, too.

  13. #163
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    1,747

    Re: Blacksmithing tools

    I don't suppose 400 degrees in the oven would be enough to soften up my "square head" Hardy.
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A

    Les

  14. #164
    Join Date
    Sep 2013
    Posts
    129

    Re: Blacksmithing tools

    Quote Originally Posted by whtbaron View Post
    I don't suppose 400 degrees in the oven would be enough to soften up my "square head" Hardy.
    Sure it will. Depends on what it's been tempered to from the beginning, though. At 400º, you might be softening it by tempering it down, but that's not very far from full hardness after a quench.




    Knives and such are often tempered somewhere between 420 and 460, depending on the alloy, and you can see how hard that leaves them. Your bolt might already be there. Honestly, I'd think it mighty odd to have such a hard bolt because that makes the bolt brittle and likely to snap rather than bend or stretch under load. Any failure would be sudden and catastrophic.

    Were it me, I'd take the torch to the head and temper it that way. Even a little hand torch with MAPP gas would have sufficient heat to get the head well beyond 400 in a few minutes. You could pre-heat it in the oven at 400, then use the propane or MAPP torch to get it up even hotter without worrying about running out of gas in those little bottles.

  15. #165
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    1,747

    Re: Blacksmithing tools

    Good idea... thanks.
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A

    Les

  16. #166
    Join Date
    Sep 2013
    Posts
    129

    Re: Blacksmithing tools

    After the expensive apron adventure, I kinda had the bug to make my own apron.

    I was very happy with the Tillman apron that I had been using, and I modeled the fancy apron after it. If the old apron hadn't dried out and started tearing, I'd still be using it today!

    So, I picked up a new Tillman 48" apron and some dye from Hobby Lobby.



    Not the best dye job I've ever seen, but I bought a second bottle of dye to, hopefully, get the thing finished and darkened enough that stains don't show up so clearly. No idea why Tillman went with that bright orange color for an apron they know will be in a metal shop!

    The weirdest thing about the dye is that it seems to evaporate rather than actually stain the leather. When freshly applied and everything wet, the apron was pretty uniform in color. When it dried out, though, this is what was left. Some spots soaked all the way through the hide. Others didn't. Splotchy would be a good description.

    The second bottle of dye performed similarly, but I think I might have solved some of the issue by putting the apron into a trash bag overnight so there wasn't anywhere for the dye to evaporate to.

    Next on the list of things to do is rivet/glue some heavier leather to the areas were the straps join the body. This is where the last apron failed, so I'm thinking it'll be a good idea to reinforce things. How will I do that? No idea.

    As much as I sweat (ain't easy being a fat man in the south!), my old attempt at using roofing nails as washers didn't last very long. It worked, but rusted to pieces in a skinny minute.

    Copper would likely do well, and I've seen brass rivets that might even be better. I figured to use some kind of rubber cement to hold the leather pieces together, but then I wondered how the glue would tolerate a light oiling.

    It's been fun so far and I think it'll work out just fine in the long run. Just gotta get the rest of the pieces together and she'll be right as rain.

    The #1 tool in my shop!

  17. #167
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    1,747

    Re: Blacksmithing tools

    What was your application method for the dye? I'm wondering if some areas were just wetter than others? Are the dark spots where it soaked through? Maybe a spray application would be more even? Maybe there was some settling within the bottles, or residues that weren't getting mixed back into solution when you shook it?
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A

    Les

  18. #168
    Join Date
    Sep 2013
    Posts
    129

    Re: Blacksmithing tools

    Quote Originally Posted by whtbaron View Post
    Maybe a spray application would be more even?
    I did use a spray bottle. My technique might not have been awesome, but I promise the whole thing was coated and looked pretty uniformly coffee-colored.

    When it dried out, this is what was left.

    The instructions on the bottle didn't say anything about wetting down the leather beforehand or shaking the bottle to mix things up. Honestly, I don't have a clue why the dye didn't soak in, or stay soaked in.

    It does look better now that I've put on a second bottle of dye. One thing I've found since the spraying, is that some bottles of dye on the market are specifically labeled as being for "suede and rough-out" leather. The stuff from Hobby Lobby doesn't say that, and I have to wonder why they'd specifically label a dye as being for suede. Maybe I bought the wrong stuff? Maybe the texture on the suede stops dyes from penetrating?

    No clue! But you can be sure that the third bottle of dye that I purchase will be specifically for suede!!!

    Next up, I'm buying a grommet kit and some extra leather. That'll reinforce the side attachment points where the straps come in. Maybe I'll get some rivets, or maybe I'll stitch the leather patches on. Not sure about that, yet.

    Getting closer, though. Once I have the system down pat, I might make a few for sale if it looks like folks'd want one for themselves. That's down the road, though.

  19. #169
    Join Date
    Sep 2016
    Location
    American Samoa
    Posts
    152

    Re: Blacksmithing tools

    Why does a fat sweaty man of the South care about fashion? Get er done!

  20. #170
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    1,747

    Re: Blacksmithing tools

    LOL... oh Dude! That's just rude! The nationally apologetic Canadian in the crowd could never say things like that... well not unless it involved beer...
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A

    Les

  21. #171
    Join Date
    Sep 2013
    Posts
    129

    Re: Blacksmithing tools

    Quote Originally Posted by Steve Shimanek View Post
    Why does a fat sweaty man of the South care about fashion?
    Gotta look good while I'm rocking it out!

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement