    My buddies 650 amp 1ph Airco Bumblebee. He paid 250$ for it on ebay. Name:  14461378524251897770334.jpg
Views: 1953
Size:  30.4 KBName:  1446137788744-798280469.jpg
Views: 1950
Size:  26.5 KBName:  145322679771525523207.jpg
Views: 1949
Size:  64.7 KBName:  14532268582621586779289.jpg
Views: 1954
Size:  62.0 KB

    Not the Airco Orange he was wanting but hes happy with it so far.
    Also have to say wow! There are some Beautiful restored machines on here! Nice work guys!!
    Airco 300
    Miller 330A/BP with Miller Radiator 1 cooler.
    RFC-23AG to share with both machines..
    Snapon YA 212
    6x10 burntable cutmaster 82
    Protools HD 105 turned vertical
    Two Big Jeeps 1 black dog and a mean wife!

  2. #27
    Join Date
    Jan 2016
    Location
    Alberta, Canada
    Posts
    3

    Re: The Welder Restoration Thread.. Post 'EM UP!

    My dad bought this old Forney at an auction sale in 1974 (I'd have been 8 years old), took it home and put it in the shed. I brought it home with me on the weekend, he's still never plugged it in.
    Electrician wired me in a 220v 50 amp receptacle in my garage today while I was at work, I went out after supper and gave it a go.

    Much to my surprise, it works like a charm. Work cable in high ground and positive in 120 and ran a few beads of 6013 1/8 on a piece of scrap. Seems to be easier to strike and hold an arc than the Thunderbolt I've been practicing with in the shop where I work. (I'm very much a beginner)

    Won't be much of a restoration though other than a wipe down, although the battery charger that chme with it needs new clamps.

    Name:  image.jpeg
Views: 1951
Size:  145.9 KB
    Last edited by Cam Stromstedt; 01-19-2016 at 11:03 PM.

  3. #28
    Join Date
    Dec 2014
    Location
    Arizona
    Posts
    39

    Re: The Welder Restoration Thread.. Post 'EM UP!

    Quote Originally Posted by mxpapa View Post
    that is a gorgeous restoration i might have to do that to mine
    Lincoln Pro Mig 180T
    Lincoln Weldanpower 225 AC/DC
    http://weldingweb.com/showthread.php...Em-Up!!/page14

  4. #29
    Join Date
    Jun 2014
    Location
    east texas
    Posts
    443

    Re: The Welder Restoration Thread.. Post 'EM UP!

    Thanks, It was fun and learned a little.Name:  00A0A_h83ddj5Z4QJ_600x450.jpg
Views: 1542
Size:  24.8 KBName:  IMG_0648.jpg
Views: 1550
Size:  63.4 KBName:  IMG_0649.jpg
Views: 1543
Size:  51.9 KB Just finished this Bluestar 2E and sold it. I like rebuilding these little welders.
    Thermal Arc 210, Tweco 211I, Cutmaster 52

  5. #30
    Join Date
    Jul 2015
    Posts
    31

    Re: The Welder Restoration Thread.. Post 'EM UP!

    Name:  20150701_210241.jpg
Views: 1472
Size:  53.2 KB
    Name:  20151019_205012.jpg
Views: 1472
Size:  45.1 KB
    Code #8399
    SA 200 Blackface Code #7307
    80's model Lincoln Weldanpower AC/DC
    Keep Calm and Weld On!
    Oklahoma State University - The STATE'S University

  6. #31
    Join Date
    Jan 2016
    Location
    Manitoba , Canada
    Posts
    71

    Re: The Welder Restoration Thread.. Post 'EM UP!

    The bar is set high , thats for sure . hope to get started on mine later this summer .
    Lots of inspiration here , thats for sure.

  7. #32
    Join Date
    May 2015
    Location
    NE Oregon
    Posts
    14

    Re: The Welder Restoration Thread.. Post 'EM UP!

    Some of us get a real charge seeing this old stuff look brand new again. Is it because when we were young we had to use worn, broken stuff all the time?

  8. #33
    Join Date
    Feb 2016
    Location
    East Texas
    Posts
    389

    Re: The Welder Restoration Thread.. Post 'EM UP!

    Quote Originally Posted by Cam Stromstedt View Post
    My dad bought this old Forney at an auction sale in 1974 (I'd have been 8 years old), took it home and put it in the shed. I brought it home with me on the weekend, he's still never plugged it in.
    Electrician wired me in a 220v 50 amp receptacle in my garage today while I was at work, I went out after supper and gave it a go.

    Much to my surprise, it works like a charm. Work cable in high ground and positive in 120 and ran a few beads of 6013 1/8 on a piece of scrap. Seems to be easier to strike and hold an arc than the Thunderbolt I've been practicing with in the shop where I work. (I'm very much a beginner)

    Won't be much of a restoration though other than a wipe down, although the battery charger that chme with it needs new clamps.

    Name:  image.jpeg
Views: 1951
Size:  145.9 KB
    I love running 7018 on my old Forney C-5 arc welder.
    Forney C5 Arc Welder
    Lincoln Idealarc 250-250 Ac/Dc Arc Welder
    Miller Bobcat 225g Plus

    Forney O/A Rig

    Dewalt D28715 14" Chop Saw



  9. #34

    Re: The Welder Restoration Thread.. Post 'EM UP!

    Name:  IMG_1264.jpg
Views: 704
Size:  58.3 KB
    any idea what year?
    thanks dave
    michigan

  10. #35
    Join Date
    Sep 2009
    Location
    Cleveland, OH USA
    Posts
    54

    Re: The Welder Restoration Thread.. Post 'EM UP!

    I have 1958/59 Sears catalog that has this welder in it $199!
    Century AC/DC 250 Amp & Midstates 300 Amp Industrial AC stick welders, Century Flux core 80 amp. wire feed welder Harris Oxy-Acet. cutting & welding outfit:
    SEE MY INFORMATIVE VIDEOS AT http://www.youtube.com/user/alpho52

  11. #36

    Re: The Welder Restoration Thread.. Post 'EM UP!

    great, thanks for the info

    dave
    michigan

  12. #37
    Join Date
    Nov 2016
    Location
    USA
    Posts
    351

    Re: The Welder Restoration Thread.. Post 'EM UP!

    [QUOTE=leightrepairs;6425681]Not to hijack this thread but Everytime i see Ceps pictures of his welder sitting on the stack of pallets i think of a jobsite i was on last year and here are a couple of pictures of the work area built by the iron workers on the job.Attachment 1252431Attachment 1252441Attachment 1252451. Always seemed odd that iron workers fab so much out of wood.

    Mike[/QUOTE

    Yeah, I see what you mean
    Last edited by eeapo; 12-03-2016 at 10:01 PM.

  13. #38

    Re: The Welder Restoration Thread.. Post 'EM UP!

    i just picked up an sa250 with the perkins for real cheap but it was a rear main seal leak. I have been looing all over and cannot find any documentation on how to split the genny from the rear of engine and I don't want to mess it up because I really love this machine but not enough to have to spend a lot of money replacing parts that I screw up. I just started a welding business so funds are a little tight until I get my tools and gear all purchased or paid off. So any assistance on this issue would be much appreciated.

  14. #39
    Join Date
    Nov 2012
    Location
    South Texas
    Posts
    2,261

    Re: The Welder Restoration Thread.. Post 'EM UP!

    Quote Originally Posted by CEP View Post
    I got a couple.
    If I ever make it back up to Washington I want to burn some 5P's with those machines just to see!

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement