    Finally Got Em:

    Received for Xmas a nice new set of Tillman 850L gloves. I guess from what she was told the Elkskin is being discontinued by Tillman as weldingsupply.com only had two pairs left in stock. I certainly like the feel and dexterity of them being as soft as they are. This is my first what I consider good pair of gloves as I've always got by with either donated, or cheap gloves so these are welcome.
    Slob

    Purveyor of intimate unparalleled knowledge of nothing about everything.

    Oh yeah, also an unabashed internet "Troll" too.....

  2. #2
    Join Date
    Apr 2016
    Location
    CA
    Posts
    3,676

    Re: Finally Got Em:

    I made the mistake of letting my left index finger get to close to the weld when stablizing my mig gun and shrunk the leather on a nice pair of gloves. Don't do that
    '65 Lincoln Idealarc 250 AC/DC
    L-tec PCM-VPi 40A plasma
    ESAB REBEL EMP 215ic
    ESAB Mig Master 250
    Victor Performer O/A

  3. #3
    Join Date
    Jul 2014
    Location
    Bulldog Heaven at the end of my chain
    Posts
    2,401

    Re: Finally Got Em:

    Yes, that is why I wanted the Elkskin. It is more resistant to the heat in regards to shrinking and stiffening up than other types of leather. I am really surprised how supple they are.
    Slob

    Purveyor of intimate unparalleled knowledge of nothing about everything.

    Oh yeah, also an unabashed internet "Troll" too.....

  4. #4
    Join Date
    Jan 2012
    Posts
    190

    Re: Finally Got Em:

    I bought two pair years ago ,wrecked the left hand glove in less than five minutes . I'll never pay that much for gloves again.

  5. #5
    Join Date
    May 2007
    Location
    SoCal
    Posts
    4,776

    Re: Finally Got Em:

    Quote Originally Posted by N2 Welding View Post
    I made the mistake of letting my left index finger get to close to the weld when stablizing my mig gun and shrunk the leather on a nice pair of gloves. Don't do that
    When I got too close to the heat, and they shrank up, I have tried immediately stretching the hot spot as far as possible while it is still hot. It helped return it to its size even if it stiffened up some. If I let it cool, it does nothing to try to stretch it back at that point. I had to pull very hard to get it to move.
    City of L.A. Structural; Manual & Semi-Automatic;
    "Surely there is a mine for silver, and a place where gold is refined. Iron is taken from the earth, and copper is smelted from ore."
    Job 28:1,2

    Lincoln, Miller, Victor & ISV Bible

    Danny

  6. #6
    Join Date
    Jul 2014
    Location
    Bulldog Heaven at the end of my chain
    Posts
    2,401

    Re: Finally Got Em:

    Used them today "playing" in the shop. Kinda like the dexterity they provide opposed to cowhide gloves. I did look on amazon and checked stock on several vendors and they seem to be readily available so don't know if my daughter was confused, or is awaiting my feedback to get me a few more pair. She does stuff like that.
    Slob

    Purveyor of intimate unparalleled knowledge of nothing about everything.

    Oh yeah, also an unabashed internet "Troll" too.....

  7. #7
    Join Date
    Jul 2014
    Location
    Kyle, TX
    Posts
    44

    Re: Finally Got Em:

    I would be surprised if they were discontinued. Seems like the most popular glove everywhere I've been.
    Sean

    Miller CST 280
    Lincoln 210 MP

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement