    welder runs and idles won't weld

    Miller Trailblazer starts runs and idles but will not weld, anyone know what it could be?

  2. #2
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,032

    Re: welder runs and idles won't weld

    Could be a number of things. Got a unit SN?

    When's the last time it welded?

    Does it make auxiliary AC power?

    Have you jump started it recently with a booster charger or off a vehicle?
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save 2nd Base!

  3. #3
    Join Date
    Dec 2016
    Location
    raleigh nc
    Posts
    454

    Re: welder runs and idles won't weld

    I had a 250g , i think it was a 84 model .
    Mine would do that sometimes right after a good tune up , the problem was when you hit the start switch battery power also had to "flash the field" in the generator. I had mine where all you had to do was bump the switch and it would be running but did not energize lone enough to flash the field . My answer to this was to pull choke and make the engine spin a few rounds before cranking .
    Also i had another problem like this with the same machine and i found bad connections where the wiring harness plugged into one of the circuit boards . My answer to this was to eliminate the plug and solder wires directly to the board . Again i cant remember the board but it was the one that delt with flashing the field when cranking.

    Maybe this will help you?

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement