    I'm thinking of buying one of these saws, however, i can not find anywhere the largest dimensions of a rectangle it will cut. Their website only says 4 1/2" at 90*. Will it cut 6" channel? Some of you guys that have this saw, if you will, help me out here. Thanks.

  2. #2
    Join Date
    Sep 2013
    Location
    central Wis.
    Posts
    2,989

    Re: Makita LC1230

    I cut some 6" flat with mine, never tried channel. It should cut it, if not it might be just a small corner it didn't cut thru.

  3. #3
    Join Date
    Dec 2016
    Posts
    21

    Re: Makita LC1230

    Thanks MJD, that is good information, good to know. Sorry to have not replied to your post sooner.

  4. #4
    Join Date
    Aug 2015
    Posts
    94

    Re: Makita LC1230

    It should I bought one and love it. Cut a bunch of schedule 40 4 inch pipe this weekend like it was pvc. Cut some tower steel that was probably 4 inch angle half inch thick no problem the cut was shiny and smooth and cool to touch immediately after the cut.


    Sent from my iPhone using Tapatalk

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement