    Those bricks you have are the right product for the job, you just need to go to a masonry supply store and buy fire glue. Fire glue is a premixed adhesive that can withstand the high temperatures unlike regular cement based products. The company that I work for built a wood burning oven in a bakery that ran 6 days a week for 8 years before the fire bricks started to deteriorate and needed to be replaced. BTW I should add that i'm a mason by trade.
    Lincoln 210 MP
    Miller Spectrum 375 X-treme Plasma
    Craftex CX600 Mill (Grizzly G0604)
    King Industrial Swivel Head Band Saw

    Welding Table Build.
    http://weldingweb.com/showthread.php...%29&highlight=

  2. #27
    Join Date
    Oct 2016
    Location
    Delavan WI
    Posts
    240

    Re: Help getting fire bricks in firebox

    Quote Originally Posted by motolife313 View Post
    He said use some hi temp cement mortor in between the blocks. Do u think cement holds to stainless steel good?
    Yes the product I was talking about hardens like glass if you don't get it off of your trowel you have to grind it off once it hardens overnight.

  3. #28
    Join Date
    Nov 2014
    Posts
    6,735

    Re: Help getting fire bricks in firebox

    I couldnt find the fire glue called 2 places.

  4. #29
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    3,229

    Re: Help getting fire bricks in firebox

    Quote Originally Posted by motolife313 View Post
    I couldnt find the fire glue called 2 places.
    Ask for refractory cement it comes premix and bagged.
    they also make something similar in a tube/ caulk gun style.
    Miller 211/Spoolmate 100
    1961 Lincoln Idealarc 250
    Hypertherm PM 45
    Lincoln SP125 plus
    HTP 221
    Chicom spot welder



    True Wisdom only comes from Pain.

  5. #30
    Join Date
    Jul 2014
    Posts
    1,955

    Re: Help getting fire bricks in firebox

    I can't remember the name brand of fire brick cement we used in the boilers ,but it came dry in a 2 1/2 gallon size bucket,we added water too it until it was almost soupy , dipped the brick on the edges we wanted bonded and laid them up with almost no mortar gap (1/8" maybe) they stayed in place nicely for years .

  6. #31
    Join Date
    Feb 2014
    Location
    Iowa
    Posts
    501

    Re: Help getting fire bricks in firebox

    Quote Originally Posted by gxbxc View Post
    I can't remember the name brand of fire brick cement we used in the boilers ,but it came dry in a 2 1/2 gallon size bucket,we added water too it until it was almost soupy , dipped the brick on the edges we wanted bonded and laid them up with almost no mortar gap (1/8" maybe) they stayed in place nicely for years .
    I had a mess trying to use it as it came (pretty mixed greenpatch), it was about consistency of peanut butter. These were partial pails left over from a job, which was given to me free. Undoubtedly it had lost some moisture from prior use, but everything I could find said not to thin, or thin very little.
    The brick sucks the moisture out so fast, and I was trying to butter the faces. I did not end up with a desirable end result.

    I ended up finding a video on YouTube of a manufacturer doing it exactly as you described (the cement literally dripped off), after I was mostly done! Needless to say the last little bit I had to do went A LOT better!

    I wouldn't have thought to thin it that much from the experience of laying block.
    Miller Dynasty 350
    Miller CP300
    Miller CP200
    Lincoln Idealarc 250/250
    Smith torch
    Lagun FTV-2
    Kent 13x40 TRL lathe
    Bunch of other metal cutting tools

  7. #32
    Join Date
    Feb 2011
    Posts
    85

    Re: Help getting fire bricks in firebox

    Dural 452 gel construction adhesive. Use it all the time in fireplaces.

  8. #33
    Join Date
    Jan 2015
    Location
    Catskills NY
    Posts
    73

    Re: Help getting fire bricks in firebox

    Nice Job moto, Did you make sure you calculated the space taken up by firebricks into your firebox size? Looks as tho theyre taking up a lot of real estate. Its important to the overall function of your reverse flow...I couldn't add bricks to mine B/C I didn't think about it before my build. However it seems to function ok without them, even using it now at our ski center on bitter cold days. Just wait till you use it and enjoy all that hard work with some awesome smoked meats...Good job!

  9. #34
    Join Date
    Mar 2014
    Posts
    5,089

    Re: Help getting fire bricks in firebox

    Concerning fire boxes in general......I don't think having the fire right on the floor (of any style of cooker/smoker fire box) is the best of ideas. What I like to do is to build a removable grate system that holds it 3 to 4 inches off the floor. And then put the air inlet damper as low as possible on the door. The idea being is that you want the inlet combustion air to come in and be able to go up thru the fire.

  10. #35
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    3,229

    Re: Help getting fire bricks in firebox

    Moto,
    put some thought into getting that thing out of the garage also.

    mine was BALLS heavy and had to weld D-rings on and hoist it with a chainfall. those bricks and 1/4" plate are heavy.
    Miller 211/Spoolmate 100
    1961 Lincoln Idealarc 250
    Hypertherm PM 45
    Lincoln SP125 plus
    HTP 221
    Chicom spot welder



    True Wisdom only comes from Pain.

  11. #36
    Join Date
    Jan 2013
    Location
    ...Shoulder of Orion...
    Posts
    3,561

    Re: Help getting fire bricks in firebox

    @ motolife313 - after your bricks are integrated, apply Heat Stop 50. Many forges use HS50 to line their castable fire bricks.
    "Discovery is to see what everybody else has seen, and to think what nobody else has thought" - Albert Szent-Gyorgyi

  12. #37
    Join Date
    Feb 2012
    Location
    Sparks, NV
    Posts
    3,484

    Re: Help getting fire bricks in firebox

    Moto, my fireplace has 2 clips (one on each side) to hold the last installed fire bricks in place. No glue.

  13. #38
    Join Date
    Nov 2014
    Posts
    6,735

    Re: Help getting fire bricks in firebox

    Needs some suggestions again, I don't really wanna put brick in the door because it will not work at easy since I wanna put holes in the door and want the door to be protected by some insulator. I'm building a stainless frame to hold in the some kind of concrete motor mix? I would then put a layer of 1/8 or 16 gauge sheet over to protect it and I plan to do the same over the insulating bricks I have so they will stay protected. Name:  image.jpg
Views: 144
Size:  55.9 KB it's not finished yet. It's 1/4 1.5" angle and 5/16 door. Thanks a lot if u have suggestion Name:  image.jpg
Views: 144
Size:  51.9 KBthis angle takes forever to cut at a 45 degree angle

  14. #39
    Join Date
    Nov 2014
    Posts
    6,735

    Re: Help getting fire bricks in firebox

    Quote Originally Posted by cloudman View Post
    I started looking around at the Smith Sharpe website and noticed they have a bunch of products for pizza ovens, outdoor fireplaces etc. They sell KILN FLOOR shiplap tiles - 12x12, 12x18, 12x24 ....
    I tried looking for them and didn't see them. I seen the fiberfrax, I looked ok.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement