    SS Filler Questions

    Haven't done SS before, have a few projects that need it now and will be buying some here shortly and very confused on which one to get.

    Only need a pound of it, which will probably last me 2-3 years. Have been looking into this and found the filler to buy is 308, but upon further reading 309 can also be used for SS to SS as well as SS to mild, buttttt upon further reading 312 is even more versatile then 308 and 309 as it can do SS to SS and everything in between while having a higher resistance to crack.

    Now, this stuff is spendy and like I said I don't do SS other then a few things here and there and would only like to buy a pound if I have to. So is there a SS filler out there that will get the job done for me? This will be used for exhaust work, coffee mugs, repairing tools, attaching things to tools, etc. Nothing structural or anything that would be holding someone life together....

  2. #2
    Join Date
    Mar 2010
    Location
    East Tennessee
    Posts
    1,145

    Re: SS Filler Questions

    312 is your friend.

  3. #3
    Join Date
    Nov 2016
    Posts
    17

    Re: SS Filler Questions

    So can 312 be used for stainless to stainless applications?

  4. #4
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    3,471

    Re: SS Filler Questions

    Last edited by Oscar; 01-06-2017 at 08:42 PM.
    First person on WeldingWeb to have a scrolling signature!

    HTP Invertig221 D.V. Water-cooled
    Millermatic 211 Inverter MIG w/ Spoolmate 150
    Eastwood 40A Plasma cutter

  5. #5
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    8,487

    Re: SS Filler Questions

    I recently learned 312 is even more corrosion resistant than 308.

    You will find it to be a more stable flowing filler as well.
    Weld like a "WELDOR", not a wel-"DERR"
    Miller Dynasty700DX, Dynasty350DX 2ea., Dynasty200DX, ThermalArc 400 GTSW, LincolnSW200 2ea., MillerMatic350P, MillerMatic200 with spoolgun, MKCobraMig260, Lincoln SP-170T,PlasmaCam/Hypertherm 1250

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement