    Hello,

    I have been a lurker here for quite awhile but figure it is about time to make a post. I don't get the opportunity to weld very often but I love it when i can. I am a diesel mechanic by trade and was wondering if you guys could critique my welds for me. These were done with a Miller Wildcat 200. First time stick welding in about 5 years.
    Name:  Weld1.jpg
Views: 48
Size:  66.5 KBName:  Weld2.jpg
Views: 45
Size:  74.2 KBName:  Weld3.jpg
Views: 50
Size:  67.6 KBName:  Weld4.jpg
Views: 49
Size:  68.9 KB

  2. #2

    Re: Hello Everyone

    Forgot to mention this was done with 7018 rod.

  3. #3
    Join Date
    May 2011
    Location
    Andover, Ohio
    Posts
    2,884

    Re: Hello Everyone

    89ranger, welcome to the forum.
    Lincoln A/C 225
    Everlast P/A 200

  4. #4
    Join Date
    Sep 2016
    Location
    American Samoa
    Posts
    118

    Re: Hello Everyone

    Howdy and welcome, welds look like they might have been a little hot; i am sure someone more qualified will be along to give a better critique.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement