    6013 looks great on AC and it's easy to run makes decent strength welds. 6011 looks ugly but it burns trough rust and oil and make decent strength welds. I made these welds with 1/16" 6013 on DC. But you should have good results on AC. I would use a 3/32" 6013 Lincoln or Hobart.The 1/16" rods are very flimsy and hard to weld with. The 3/32" is stiff enough and wont blow trough 1/8" wall as easy a 6011.

    Name:  6013 lincoln new cut.jpg
Views: 160
Size:  20.8 KB

    I would use a 3/16" for all of it. It's not that much more expensive and it won't rust out as fast. It's also a lot stronger. 1/8" is strong enough but it will flex a lot more than 3/16". How far apart are you connecting legs? The part that go's from the handrail to the flat plate.
    Last edited by 69sa200; 01-10-2017 at 10:37 PM.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement