    Re: Hypertherm Powermax 30XP?

    That's cool, you certainly won't regret getting the 45 over the 30. The 45 will give you the ability to gouge. This means that when , not if you make an inferior weld you can easily remove it . Make sure and do a review on the 45xp when you get it up and running.

  2. #127
    Join Date
    May 2016
    Location
    Camarillo, CA
    Posts
    142

    Re: Hypertherm Powermax 30XP?

    Sure. I'll do a Youtube review on it on my Youtube channel and of course thank you guys in the process. I promise.
    Hobart Handler 190
    Hypertherm Powermax 45XP
    Welder12 on Youtube: https://www.youtube.com/channel/UCMd...BGgVPbze3Kic3w

  3. #128
    Join Date
    Jul 2015
    Location
    Central Florida
    Posts
    140

    Re: Hypertherm Powermax 30XP?

    So why are you at home playing around on the computer??? You should be out cutting grass and helping little old ladies cross the street for tips! lmao
    Millermatic 180

    Hypertherm PM65 083300
    CandCNC Dragon Cut Linux 620-4 Bundle with Linux Computer
    Precision Plasma Magnum HD 5x5 Gantry kit

  4. #129
    Join Date
    Oct 2006
    Location
    Illinois
    Posts
    8,234

    Re: Hypertherm Powermax 30XP?

    Quote Originally Posted by Ovrrdrive View Post
    So why are you at home playing around on the computer??? You should be out cutting grass and helping little old ladies cross the street for tips! lmao
    Keith has advanced to SUPERVISOR/OWNER . He hired a young guy for $5.00 a hour to cut grass that he charges $20.00 a hour for.

    See , I knew He was the real deal !

  5. #130
    Join Date
    May 2016
    Location
    Camarillo, CA
    Posts
    142

    Re: Hypertherm Powermax 30XP?

    Does the 45XP have a built in air dryer? Or would I have to but one. And if so, does the dryer take consumables or is it a coalescing filter? Thanks
    Hobart Handler 190
    Hypertherm Powermax 45XP
    Welder12 on Youtube: https://www.youtube.com/channel/UCMd...BGgVPbze3Kic3w

  6. #131
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    2,589

    Re: Hypertherm Powermax 30XP?

    Quote Originally Posted by Keith Merrell View Post
    Does the 45XP have a built in air dryer? Or would I have to but one. And if so, does the dryer take consumables or is it a coalescing filter? Thanks
    It has a small water separator inside.

    But You will need more ... motorgard m60


    Sent from my iPhone using Tapatalk
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  7. #132
    Join Date
    Oct 2007
    Location
    New Hampshire
    Posts
    3,128

    Re: Hypertherm Powermax 30XP?

    In 95% of the installations of Powermax systems there is no need whatsoever for additional filtration or moisture / oil separation. The 45 XP has a particulate filter (replaceable element) as well as a coalescing moisture / oil separator with an auto drain. If you have high enough moisture levels to get to the coalescer....then you will see signs of moisture in the clear bowl. Usually you won't.....especially where Keith's system will be used in the relatively low humidity part of the U.S. (CA). I suggest to Keith (and everyone else with a plasma) to drain the compressor tank daily....better yet install an auto drain.

    There is so much hype online about how moisture dramatically affects cut quality with a plasma cutter.....and with older technology plasma cutters (as well as with low cost imports that use copies of older technology) this can be true. The latest generations of Hypertherm Powermax units will tolerate trace amounts of moisture (not oil though!). Moisture in compressed air is enhanced by the local humidity, by high duty cycles (compressor getting hot and running continuously) and by allowing the tank to collect water. I doubt that Keith will experience much of any of this! Jim Colt Hypertherm




    Quote Originally Posted by Keith Merrell View Post
    Does the 45XP have a built in air dryer? Or would I have to but one. And if so, does the dryer take consumables or is it a coalescing filter? Thanks

  8. #133
    Join Date
    Oct 2006
    Location
    Illinois
    Posts
    8,234

    Re: Hypertherm Powermax 30XP?

    Here is another reply by Jim Colt about air. Check this out too, http://weldingweb.com/showthread.php...evel-cnc-table

    POST # 12 is where he writes about AIL LINE SIZE

  9. #134
    Join Date
    May 2016
    Location
    Camarillo, CA
    Posts
    142

    Re: Hypertherm Powermax 30XP?

    Got a package from psacustomcreations. There was a check and a bunch of safety gear inside. Tons of earplugs, respirators, goggles, gloves, safety glasses, filters, and a bunch of other stuff. Thanks a lot man!!! Letter sent.
    Hobart Handler 190
    Hypertherm Powermax 45XP
    Welder12 on Youtube: https://www.youtube.com/channel/UCMd...BGgVPbze3Kic3w

  10. #135
    Join Date
    Apr 2015
    Location
    Fredericksburg, VA
    Posts
    837

    Re: Hypertherm Powermax 30XP?

    Quote Originally Posted by Keith Merrell View Post
    Got a package from psacustomcreations. There was a check and a bunch of safety gear inside. Tons of earplugs, respirators, goggles, gloves, safety glasses, filters, and a bunch of other stuff. Thanks a lot man!!! Letter sent.
    No problem. Post a pic if you have a chance of that and the rest of your gear so others might be able to help you out.

    Like I said, make sure you use the safety gear. Ask anyone on this thread or even on the whole site how many times they have gotten something in their eye, grabbed a hot piece of metal, cut themselves, or breathed a bunch of bad fumes. Start out developing some good safety habits now. Ignore those who ay you need to be a tough guy and not wear safety gear.

    Sent from my SM-G930V using Tapatalk
    Millermatic 252 MIG
    Miller Dynasty 200DX TIG
    Miller Spectrum 375 Plasma
    Altas 12x36 Metal Lathe
    Bridgeport Milling Machine
    www.psacustomcreations.com

  11. #136
    Join Date
    May 2016
    Location
    Camarillo, CA
    Posts
    142

    Re: Hypertherm Powermax 30XP?

    Always wear my safety glasses in the shop, ear protection when it gets loud, and a respirator when I use the wire wheel or that abrasive Makita chop saw that spits yummy fiberglass everywhere. I'll post some pics soon.
    Hobart Handler 190
    Hypertherm Powermax 45XP
    Welder12 on Youtube: https://www.youtube.com/channel/UCMd...BGgVPbze3Kic3w

  12. #137
    Join Date
    Feb 2016
    Location
    Myrtle Beach
    Posts
    210

    Re: Hypertherm Powermax 30XP?

    Got you're letter today Kieth you're welcome and I wish you the best of luck!
    Lincoln 350MP
    Millermatic 350P
    Syncrowave 250
    1969 SA200

  13. #138
    Join Date
    May 2016
    Location
    Camarillo, CA
    Posts
    142

    Re: Hypertherm Powermax 30XP?

    Name:  SAM_4316.jpg
Views: 122
Size:  70.9 KB This is what psacustomcreations sent. Thats not all of it either. Thanks psa!
    Hobart Handler 190
    Hypertherm Powermax 45XP
    Welder12 on Youtube: https://www.youtube.com/channel/UCMd...BGgVPbze3Kic3w

  14. #139
    Join Date
    Oct 2006
    Location
    Illinois
    Posts
    8,234

    Re: Hypertherm Powermax 30XP?

    That's GREAT Keith ! You are gonna need a gang box for all your goodies .

  15. #140
    Join Date
    Sep 2013
    Location
    central Wis.
    Posts
    3,442

    Re: Hypertherm Powermax 30XP?

    Received your letter today . Your welcome , when you get your machine, be safe. Good luck to you.

  16. #141
    Join Date
    Jul 2015
    Posts
    22

    Re: Hypertherm Powermax 30XP?

    well have you bought the Hypertherm yet?

  17. #142
    Join Date
    Jan 2008
    Location
    Richmond, Virginia
    Posts
    6,833

    Re: Hypertherm Powermax 30XP?

    Quote Originally Posted by BD1 View Post
    ... You are gonna need a gang box for all your goodies .
    I had to build a "gang box" about 15 years ago. 30 ft. x 30 ft, 2 stories. But it's full now!
    "USMCPOP" First-born son: KIA Iraq 1/26/05
    Syncrowave 250 w/ Coolmate 3
    Dialarc 250, Idealarc 250
    SP-175 +
    Firepower TIG 160S (gave the TA 161 STL to the son)
    Lincwelder AC180C (1952)
    Victor & Smith O/A torches
    Miller spot welder

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement