TIG Helmet-Mask Settings
RSS | Subscribe | Contact Us | Advertise | About Us
Results 1 to 15 of 15
  1. #1
    Join Date
    Dec 2015
    Posts
    14

    TIG Helmet-Mask Settings

    Just learning to TIG.

    Have a nice Lincoln-Viking 3350 series auto-darkening helmet.

    What is the lightest SHADE setting I can use to TIG?
    (want to see as much as possible while learning on 1/8" aluminum)

    And can someone explain the SHADE 5-8 and SHADE 9-13 switches and corresponding SHADE wheel settings?

    Thanks!

  2. #2
    Join Date
    Feb 2009
    Location
    Chicago
    Posts
    6,089

    Re: TIG Helmet-Mask Settings

    Depends on your amperage and your eyes. Everyone likes it differently.
    I like mine at shade 9 up to 200 amps. But it will vary from person to person.
    Torchmate 2x2 CNC with Flashcut CNC controls
    Hypertherm Powermax45
    2015 AHP Tig
    Razorweld 195 Mig
    Razorweld 200ac/dc Tig
    ViperMig 180
    Razorweld, SSC Foot Pedal & MK Products & Atlas Positioner Dealer

  3. #3
    Join Date
    Jan 2006
    Location
    In A Nice Comfy Chair
    Posts
    18,696

    Re: TIG Helmet-Mask Settings

    Mine is either up or down.


    ...zap!


    I am not completely insane..
    Some parts are missing

    Professional Driver on a closed course....
    Do not attempt.

    Just because I'm a dumbass don't mean that you can be too.
    So DON'T try any of this **** l do at home.

  4. #4
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    8,499

    Re: TIG Helmet-Mask Settings

    AC welding is a bright process. I prefer shade 10 myself. Too bright and I get eye fatigue. Too dark and I loose focus.

    If you have a Harbor Frieght autodark, remember to peel the protective film off.
    Weld like a "WELDOR", not a wel-"DERR"
    Miller Dynasty700DX, Dynasty350DX 2ea., Dynasty200DX, ThermalArc 400 GTSW, LincolnSW200 2ea., MillerMatic350P, MillerMatic200 with spoolgun, MKCobraMig260, Lincoln SP-170T,PlasmaCam/Hypertherm 1250

  5. #5
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    3,472

    Re: TIG Helmet-Mask Settings

    What you don't want:



    What you do want (or at least as close as possible to it----you want to be be able to just barely distinguish the tip of the tungsten from the arc light).
    First person on WeldingWeb to have a scrolling signature!

    HTP Invertig221 D.V. Water-cooled
    Millermatic 211 Inverter MIG w/ Spoolmate 150
    Eastwood 40A Plasma cutter

  6. #6
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    5,601

    Re: TIG Helmet-Mask Settings

    I'm on shade 10 most the time

  7. #7
    Join Date
    Oct 2015
    Location
    Joliet, IL
    Posts
    800

    Re: TIG Helmet-Mask Settings

    You set it to what you want. Every shade is 100% UV protection. Brighter doesn't hurt your eyes, it can just increase fatigue. So just set your hood to what you're comfortable with.

  8. #8
    Join Date
    Jul 2008
    Posts
    1,591

    Re: TIG Helmet-Mask Settings

    I like it as dark as I can get it and still see. Right now, I use a fixed shade #11 except for tacking, when I use an AD. As my eyes wear out, I expect to have to make it brighter, so the longer I can stick with #11, the better. If you're like me, you'll find that you can see the puddle A LOT better with a fixed shade than with an autodark.

  9. #9
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    8,499

    Re: TIG Helmet-Mask Settings

    Quote Originally Posted by Kelvin View Post
    I like it as dark as I can get it and still see. Right now, I use a fixed shade #11 except for tacking, when I use an AD. As my eyes wear out, I expect to have to make it brighter, so the longer I can stick with #11, the better. If you're like me, you'll find that you can see the puddle A LOT better with a fixed shade than with an autodark.
    Yup. I am the same way. Nothing beats my fixed Phillips Safety glass gold lens.
    Weld like a "WELDOR", not a wel-"DERR"
    Miller Dynasty700DX, Dynasty350DX 2ea., Dynasty200DX, ThermalArc 400 GTSW, LincolnSW200 2ea., MillerMatic350P, MillerMatic200 with spoolgun, MKCobraMig260, Lincoln SP-170T,PlasmaCam/Hypertherm 1250

  10. #10
    Join Date
    Jul 2008
    Location
    Long Island
    Posts
    2,864

    Re: TIG Helmet-Mask Settings

    Quote Originally Posted by JESFromRIC View Post
    Just learning to TIG.

    Have a nice Lincoln-Viking 3350 series auto-darkening helmet.

    What is the lightest SHADE setting I can use to TIG?
    (want to see as much as possible while learning on 1/8" aluminum)

    And can someone explain the SHADE 5-8 and SHADE 9-13 switches and corresponding SHADE wheel settings?

    Thanks!
    Not owning your helmet, my guess is 5-8 is for gas welding or plasma cutting, while 9-13 is what you would want for TIG. What does your instruction manual say?

    Anywhere from 9 and up should be safe for TIG welding (at all but extreme currents) with an auto-darkening helmet, but the shade you should use would be the one you are most comfortable with. Too light, and your eyes fatigue (as stated above) and you see spots that make the puddle hard to see clearly. Aluminum is quite reflective, so I'd probably be using shade 10 or 11 on my helmet in your situation (though not all helmet's shade numbers are perfectly calibrated to each other).

    Do you have blue eyes? Blue eyes can be more sensitive to bright light, and people with blue eyes often prefer one shade darker than people with brown (like myself).

  11. #11
    Join Date
    Dec 2015
    Posts
    14

    Re: TIG Helmet-Mask Settings

    Thanks All!
    Sorry, didn't get post notification.
    10 it shall be!
    And, thanks for the great pictures too.

  12. #12
    Join Date
    Mar 2015
    Location
    usa
    Posts
    73

    Re: TIG Helmet-Mask Settings

    alot of it also depends on the lens. at home i use jackson w60 trusight and can see just fine at 150a with shade 11. other lower qaulity lenses ive had to use lower shades and still cant see nearly as well .

  13. #13
    Join Date
    Dec 2016
    Location
    Cape Coral, FL
    Posts
    53

    Re: TIG Helmet-Mask Settings

    I also have a Lincoln 3350 helmet, I use #9 most of the time, or #10 while doing aluminum due to the higher current and brighter arc. Nice helmet BTW! As stated above the lower shades are for grinding, etc.

  14. #14
    Join Date
    Aug 2016
    Posts
    58

    Re: TIG Helmet-Mask Settings

    Got that Lincoln too, using for several months. Great helmet!

    Hard to understand how there are numerous shade settings, with this thingy.

    Like 2 circles of settings, one knob.

    Name:  P1010745.jpg
Views: 179
Size:  47.8 KB



    Charl

  15. #15
    Join Date
    Dec 2015
    Posts
    14

    Re: TIG Helmet-Mask Settings

    Quote Originally Posted by xmmancharl View Post
    Got that Lincoln too, using for several months. Great helmet!

    Hard to understand how there are numerous shade settings, with this thingy.

    Like 2 circles of settings, one knob.

    Name:  P1010745.jpg
Views: 179
Size:  47.8 KB

    Charl
    OK
    So not just me then.
    The manual is no help either.
    I have the upper switch set to the higher number range and set on the 10 between 6 and 5 on the dial switch shown.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement