    Quote Originally Posted by mad welder 4 View Post
    Also try running a purely resistive load like a 100w or bigger halogen or incandescent light on each line. It can help clean up those transient spikes some times.
    That seems like a good idea to try!! I remember when we used to run an emergency tractor Pto cenerator to power the dairy
    and was told not to run it idle Always have something using a little power Like a light bulb
    I will try that! Thanks

  2. #27
    Join Date
    Nov 2014
    Posts
    152

    Re: 181 i NOT GENERATOR COMPATABLE

    Quote Originally Posted by Birdhunter1 View Post
    Is the Powerhorse clean enough to run my PA 200ST?


    Sent from my iPhone using Tapatalk
    Yes. The Powerhorse brand of gen. have less than 5%THD. A very expensive ( in my eyes) Generac GP has as much as 20%THD.

  3. #28
    Join Date
    Nov 2008
    Location
    south GA where its hot in summer and cold in winter
    Posts
    4,767

    Re: 181 i NOT GENERATOR COMPATABLE

    Quote Originally Posted by Birdhunter1 View Post
    Is the Powerhorse clean enough to run my PA 200ST?


    Sent from my iPhone using Tapatalk
    Absolutely. Unless there is something wrong with the generator. I know many customers have bought and used them successfully.
    Esab Migmaster 250
    Lincoln SA 200
    Lincoln Ranger 8
    Smith Oxy Fuel setup
    Everlast PowerPlasma 80
    Everlast Power iMIG 160
    Everlast Power iMIG 205
    Everlast Power iMIG 140E
    Everlast PowerARC 300
    Everlast PowerARC 140ST
    Everlast PowerTIG 255EXT

  4. #29
    Join Date
    Nov 2008
    Location
    south GA where its hot in summer and cold in winter
    Posts
    4,767

    Re: 181 i NOT GENERATOR COMPATABLE

    Quote Originally Posted by lugweld View Post
    Absolutely. Unless there is something wrong with the generator. I know many customers have bought and used them successfully.
    A combination like this is much less expensive, more convenient and more capable than a small generator welder that costs 2 to 3 times as much. It's an out of the box idea that makes a lot of pros cringe, but it works and does a competent job. And the generator and a welder, with a 9000w of power and 200 amps of stick welding power can do a lot.
    Esab Migmaster 250
    Lincoln SA 200
    Lincoln Ranger 8
    Smith Oxy Fuel setup
    Everlast PowerPlasma 80
    Everlast Power iMIG 160
    Everlast Power iMIG 205
    Everlast Power iMIG 140E
    Everlast PowerARC 300
    Everlast PowerARC 140ST
    Everlast PowerTIG 255EXT

  5. #30
    Join Date
    Mar 2011
    Posts
    127

    Re: 181 i NOT GENERATOR COMPATABLE

    Hi Everyone, I Thought I should pass on what I discovered!
    When I tested the power output from the extension lead It was reading way too high! 260v
    Throttled the engine back a bit until it was reading 220v And "Know What" the welder worked perfectly,
    So I was very happy with that At least the high power didn't harm the welder
    Thanks everyone for the replies

  6. #31
    Join Date
    Jun 2012
    Location
    Bemidji MN
    Posts
    13,816

    Re: 181 i NOT GENERATOR COMPATABLE

    Quote Originally Posted by Josey View Post
    Hi Everyone, I Thought I should pass on what I discovered!
    When I tested the power output from the extension lead It was reading way too high! 260v
    Throttled the engine back a bit until it was reading 220v And "Know What" the welder worked perfectly,
    So I was very happy with that At least the high power didn't harm the welder
    Thanks everyone for the replies
    Good to hear the fix was simple.
    The welder likely wouldn't weld because the incoming power was out of range - computer saved itself.
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Airco 300 - Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  7. #32
    Join Date
    Oct 2011
    Location
    Hamlin, NY
    Posts
    1,214

    Re: 181 i NOT GENERATOR COMPATABLE

    Quote Originally Posted by tkevan View Post
    Yes. The Powerhorse brand of gen. have less than 5%THD. A very expensive ( in my eyes) Generac GP has as much as 20%THD.
    Yeah, I find that today a lot of generators there is no correlation between price/brand and quality anymore. Just depends which shift in China your generator head was wound by.
    Ryan

    Miller Multimatic 200 tig/spool gun/wireless remote
    Millermatic 350P, Bernard/XR Python guns
    Miller Dynasty 350, Coolmate 3.5 & wireless remote
    CK WF1 TIG wire feeder
    Miller Spectrum 375 Xtreme
    Optrel e684
    Miller Digital Elite
    Miller Weld-Mask

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement