    So a guy called me, and asked if I could build him some h-brace for vines to grow on. I said yes, and he gave me a deposit for the metal. I'm building 9 h braces at the moment, and if he like them he might need over 300 of them!!! Name:  IMG_0727.jpg
Views: 1679
Size:  103.2 KB So me and my dad went and got the metal last weekend. Name:  IMG_0729.jpg
Views: 1677
Size:  69.7 KB Then I took my time, to get the first one perfect so I had a plan. Name:  IMG_2916.jpg
Views: 1676
Size:  66.0 KB Yesterday and today I got all the verticals cut to 10' when I got home from school . My goal is to get the horizontals cut down to 5' tomorrow and Thursday after school. Then torch cut all the saddles by Saturday morning. After that I will just fit them and weld them all weekend. I will keep posting pictures along the way.
    Forney C5 Arc Welder
    Lincoln Idealarc 250-250 Ac/Dc Arc Welder
    Miller Bobcat 225g Plus
    Lincoln PowerMig 200

    Forney O/A Rig




  2. #2
    Join Date
    Feb 2016
    Location
    East Texas
    Posts
    384

    Re: First Paid Welding Gig

    Sorry for the phone tilt here it is tilted. Name:  IMG_0731.jpg
Views: 1663
Size:  64.2 KBName:  IMG_0731.jpg
Views: 1663
Size:  64.2 KB
    Forney C5 Arc Welder
    Lincoln Idealarc 250-250 Ac/Dc Arc Welder
    Miller Bobcat 225g Plus
    Lincoln PowerMig 200

    Forney O/A Rig




  3. #3
    Join Date
    Oct 2006
    Location
    Illinois
    Posts
    8,483

    Re: First Paid Welding Gig

    What are you using to set these up on ??? Something like this could be productive if you set up a jig to set them up in. you could even make a couple of wood saw horses . Anything to make them the same without doing any additional measuring.
    What size is the pipe or tube ???

  4. #4
    Join Date
    Nov 2012
    Location
    South Texas
    Posts
    2,127

    Re: First Paid Welding Gig

    What kind of vines is he growing in East Texas?

  5. #5
    Join Date
    Feb 2016
    Location
    East Texas
    Posts
    384

    Re: First Paid Welding Gig

    Quote Originally Posted by BD1 View Post
    What are you using to set these up on ??? Something like this could be productive if you set up a jig to set them up in. you could even make a couple of wood saw horses . Anything to make them the same without doing any additional measuring.
    What size is the pipe or tube ???
    I'm setting them up on the garage floor with corner clamps to get some tacks on them,I also put a saddled 5' piece at the end to keep it from sucking in. I keep the smoke out of the garage with a big TSC fan, sucking the smoke out (works really good). I'm planing on cutting some 2x4's up so I can space the cross members with out additional measuring. I am using 2 3/8 drill stem pipe.


    Sent from my iPhone using Tapatalk
    Forney C5 Arc Welder
    Lincoln Idealarc 250-250 Ac/Dc Arc Welder
    Miller Bobcat 225g Plus
    Lincoln PowerMig 200

    Forney O/A Rig




  6. #6
    Join Date
    Feb 2016
    Location
    East Texas
    Posts
    384

    Re: First Paid Welding Gig

    Quote Originally Posted by TimmyTIG View Post
    What kind of vines is he growing in East Texas?
    I'm not sure. He said he was getting some developed at a college in California. I'll ask him next time I talk to him.


    Sent from my iPhone using Tapatalk
    Forney C5 Arc Welder
    Lincoln Idealarc 250-250 Ac/Dc Arc Welder
    Miller Bobcat 225g Plus
    Lincoln PowerMig 200

    Forney O/A Rig




  7. #7
    Join Date
    Oct 2006
    Location
    Illinois
    Posts
    8,483

    Re: First Paid Welding Gig

    Corner clamps make it really nice. I did a job and the BESSEY WELDERS clamps paid for themselves.
    Make up some saw horse or get some old tables to set up on, it will be easier on your body. That's perfect for making a jig to make life easier , quicker, and safer. Hope it all works out.
    As for the saddles , you can make a template for marking. That would help too if you haven't done that already.

  8. #8
    Join Date
    May 2010
    Location
    Port Orchard, WA.
    Posts
    9,744

    Re: First Paid Welding Gig

    If you have a drill press, I would use a hole saw to saddle the pipe. Less clean up.
    Attached Images Attached Images   
    Don’t pay any attention to me
    I’m just a hobbyist!

    Carl

    Dynasty 300
    V350-Pro w/pulse
    SG Spool gun
    1937 IdealArc-300
    PowerArc 200ST
    3 SA-200s
    Vantage 400





  9. #9
    Join Date
    Oct 2015
    Location
    PNW
    Posts
    319

    Re: First Paid Welding Gig

    maybe forget the saddle all together?

    depending on wall thickness it may be effective to just flatten the ends with a couple hits with a sledge.

  10. #10
    Join Date
    Jan 2014
    Location
    First state
    Posts
    115

    Re: First Paid Welding Gig

    Quote Originally Posted by tracymobilecnc View Post
    maybe forget the saddle all together?

    depending on wall thickness it may be effective to just flatten the ends with a couple hits with a sledge.
    He's being paid to fab these. IMHO, the customer should expect (and get) professional results. Seems to me that sledge hammering the ends would lead to distorting, undesired bending, and inconsistent results.

    I like the idea of the drill press, or he could fab a drill jig with some steel plate. Clamp the pipe, and drill thru the a guide hole, to saddle the end if the work piece.
    Millermatic 180 Mig
    Lincoln IdealArc 250
    Thermal Dynamics Cutmaster 42
    Cut50 Plasma cutter
    Craftsman(1980) buzzbox

  11. #11
    Join Date
    Oct 2015
    Location
    PNW
    Posts
    319

    Re: First Paid Welding Gig

    Quote Originally Posted by Will S. View Post
    He's being paid to fab these. IMHO, the customer should expect (and get) professional results. Seems to me that sledge hammering the ends would lead to distorting, undesired bending, and inconsistent results.

    I like the idea of the drill press, or he could fab a drill jig with some steel plate. Clamp the pipe, and drill thru the a guide hole, to saddle the end if the work piece.
    being paid or not there's nothing un-professional about flattening the ends its commonly done in many applications. a hammer is just an example, and somthing that i have done professionally. could just as well put the end in a press.

    coping the ends is a time consuming process, and often necessary but in this application and potential quantity the time savings may yield a better value for the farmer and more profit for the fabricator. which is why it may be worth considering.

  12. #12
    Join Date
    Mar 2014
    Posts
    4,477

    Re: First Paid Welding Gig

    IDK guys he's talking about using 2 3/8 drill stem. Hammering them flat or using a hole saw to cut a saddle sounds like a hard and inefficient way to go about it to me. I'd say he get one of those fancy metal hinged templates, mark'em out and go at it with a cutting torch. If this is a younger, less experienced hand it sounds like this job would be a good opportunity for him to practice and develope his manual torch cutting skills.

  13. #13
    Join Date
    Feb 2016
    Location
    East Texas
    Posts
    384

    Re: First Paid Welding Gig

    Quote Originally Posted by BD1 View Post
    Corner clamps make it really nice. I did a job and the BESSEY WELDERS clamps paid for themselves.
    Make up some saw horse or get some old tables to set up on, it will be easier on your body. That's perfect for making a jig to make life easier , quicker, and safer. Hope it all works out.
    As for the saddles , you can make a template for marking. That would help too if you haven't done that already.
    The corner clamps come in handy, and I have one of those red coping templates that open up. I have done coping from building fire wood racks and a drag harrow out of this pipe . (I'll post the firewood racks don't know why I haven't though.)


    Sent from my iPhone using Tapatalk
    Forney C5 Arc Welder
    Lincoln Idealarc 250-250 Ac/Dc Arc Welder
    Miller Bobcat 225g Plus
    Lincoln PowerMig 200

    Forney O/A Rig




  14. #14
    Join Date
    Feb 2016
    Location
    East Texas
    Posts
    384

    Re: First Paid Welding Gig

    I'm going to torch cut the saddles, so I might be as good as some of you with a torch someday. I think hole saws would take forever on drill stem, because it's close to 1/4". Thanks for all the replies, I really appreciate it. Will get some more pictures soon.


    Sent from my iPhone using Tapatalk
    Forney C5 Arc Welder
    Lincoln Idealarc 250-250 Ac/Dc Arc Welder
    Miller Bobcat 225g Plus
    Lincoln PowerMig 200

    Forney O/A Rig




  15. #15
    Join Date
    May 2010
    Location
    Port Orchard, WA.
    Posts
    9,744

    Re: First Paid Welding Gig

    I’ve never tried saddling with a chop saw. Someone posted this. If I remember correctly he built a lot of pipe fences.
    Attached Images Attached Images  
    Don’t pay any attention to me
    I’m just a hobbyist!

    Carl

    Dynasty 300
    V350-Pro w/pulse
    SG Spool gun
    1937 IdealArc-300
    PowerArc 200ST
    3 SA-200s
    Vantage 400





  16. #16
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    5,589

    Re: First Paid Welding Gig

    Have u tried it on ur bandsaw CEP?

  17. #17
    Join Date
    May 2010
    Location
    Port Orchard, WA.
    Posts
    9,744

    Re: First Paid Welding Gig

    Quote Originally Posted by motolife313 View Post
    Have u tried it on ur bandsaw CEP?
    No I haven’t. What little pipe I saddle, I use my mil with hole saws or annual cutters.
    Don’t pay any attention to me
    I’m just a hobbyist!

    Carl

    Dynasty 300
    V350-Pro w/pulse
    SG Spool gun
    1937 IdealArc-300
    PowerArc 200ST
    3 SA-200s
    Vantage 400





  18. #18
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    3,009

    Re: First Paid Welding Gig

    I would flatten, if I had a device to consistently and efficiently produce results. Coping with a saw would probably be the way I do it, since it is the way I currently do pipe. Cope would allow you to use corner jigs while flattening might make it difficult. Though- the first should be your jig for the rest.

    Hole saw...I have had a jd2 coper 5 years, have never use on tubing. It adds another operation and slows me down.

  19. #19
    Join Date
    Oct 2016
    Posts
    157

    Re: First Paid Welding Gig

    If I'm making a couple joints that require coping, ill use my portable bandsaw and notch the pipe. If I'm making a bunch of gates or something, ill get the chop saw out and set it at about 30 degrees and use that. Just leave a little flat part (larger for bigger pipe) so the miters dont come to a point. It makes a damn close fitting that is easy to weld up. But, I understand OP wants to get better with a torch, so have at it!
    '82 SA 200
    Ranger 8
    HH 140EZ
    Ironman 230

  20. #20
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    3,009

    Re: First Paid Welding Gig

    There are some nice DIY hole saw jigs on this forum. Wroughtnharv had a technique where he cut 1/4" piece of tube. Hammered it onto the face of the vertical tube and ran the horizontal tube through the formed saddle that was formed. Slick

  21. #21
    Join Date
    Nov 2012
    Location
    South Texas
    Posts
    2,127

    Re: First Paid Welding Gig

    I do those with a 4 inch grinder. Set your flat end up against where you want to saddle on, see how much gap there is, grind a straight notch that deep 180 degrees apart on your flat end. Wallow out what you need to make it fit with the grinder, round off the corners, done! Once you do a couple of them you'll get the hang of it.

  22. #22
    Join Date
    Feb 2016
    Location
    East Texas
    Posts
    384

    Re: First Paid Welding Gig

    Quote Originally Posted by CEP View Post
    I’ve never tried saddling with a chop saw. Someone posted this. If I remember correctly he built a lot of pipe fences.
    I might try that.


    Sent from my iPhone using Tapatalk
    Forney C5 Arc Welder
    Lincoln Idealarc 250-250 Ac/Dc Arc Welder
    Miller Bobcat 225g Plus
    Lincoln PowerMig 200

    Forney O/A Rig




  23. #23
    Join Date
    May 2010
    Location
    Port Orchard, WA.
    Posts
    9,744

    Re: First Paid Welding Gig

    Quote Originally Posted by Jess View Post
    I might try that.


    Sent from my iPhone using Tapatalk
    If you do, let us know how it works. Picture would be great.
    Don’t pay any attention to me
    I’m just a hobbyist!

    Carl

    Dynasty 300
    V350-Pro w/pulse
    SG Spool gun
    1937 IdealArc-300
    PowerArc 200ST
    3 SA-200s
    Vantage 400





  24. #24
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    1,700

    Re: First Paid Welding Gig

    Quote Originally Posted by CEP View Post
    I’ve never tried saddling with a chop saw. Someone posted this. If I remember correctly he built a lot of pipe fences.
    This is what I did before I bought a tubing notcher, works great, it's easy and fast.

  25. #25
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    1,700

    Re: First Paid Welding Gig

    Congrats on landing the job, are you painting the braces too?

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement