    Found this on Pinterest and I'm assuming the art has been tigged. But how did he get those colors and control where they went?
    Attached Images Attached Images    

  2. #2
    Join Date
    Dec 2016
    Posts
    225

    Re: How did he get these colors in his welds?

    Heat and penetration.


    Sent from my iPhone using Tapatalk

  3. #3
    Join Date
    Nov 2012
    Location
    South Texas
    Posts
    2,131

    Re: How did he get these colors in his welds?

    If you wash over stainless without adding wire you will get those colors.

  4. #4
    Join Date
    Oct 2007
    Location
    Vandalia, Ohio near Dayton
    Posts
    2,461

    Re: How did he get these colors in his welds?

    The color comes from oxygen reacting with the the metal surface when the surface is still hot. This can happen accidentally by allowing air to contaminate the shielding gas while welding.

    I think TimmyTIG is right. The artist heated the material using a TIG torch, without adding filler metal, and allowed some air to contact the metal while it was still hot. The temperature of the base metal determines the color of the oxide film formed.

    There are some artists doing this with Titanium to make some wild colors on jewelry.
    Benson's Mobile Welding at your worksite or place of business. Serving Dayton, Ohio and the surrounding metro areas.
    AWS Certified Welding Inspector (#XXX10731) and Certified Welding Educator (#XXX1008E)

  5. #5
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    5,592

    Re: How did he get these colors in his welds?

    That little guy at the bottom is sweet, any idea how much they go for, a Hundo maybe?

  6. #6
    Join Date
    Jan 2015
    Location
    Ohio
    Posts
    315

    Re: How did he get these colors in his welds?

    Very interesting. So he probably completely built the piece first, then used the torch here and there at different temperatures.

    If heat determines the color, how did he go from base metal to yellow,orange,red in one place and then in another place go from base metal to light blue then dark blue? I'm wondering if he applied some sort of coating that changed the color sequence.

    @motolife313
    He sells some stuff on Etsy. He has a Darth Maul face on there for $199. He's a 23 yr old engineer from Chicago - Richard Lauth. https://www.etsy.com/shop/JackWeld?z...ontent=2147023 More at: https://creativitism.wordpress.com/2...the-metal-man/
    Last edited by JD1; 01-11-2017 at 01:27 PM.

  7. #7
    Join Date
    Nov 2012
    Location
    South Texas
    Posts
    2,131

    Re: How did he get these colors in his welds?

    At the start of the bead where the metal is the coolest, you get a platinum like or silver color. As the metal heats up, the color changes to blue. It all depends on the temp of the base metal what color you get.

  8. #8
    Join Date
    Jan 2008
    Location
    Richmond, Virginia
    Posts
    6,921

    Re: How did he get these colors in his welds?

    One might get one of those little tiny Smith O/A torches (Little Torch) just to put the finishing touches on an art piece. Might be a little easier to see and control color. Just a thought.

    I'm still trying to figure out this guy's technique for a finely crafted art piece.

    Name:  by johan art.jpg
Views: 259
Size:  29.1 KB

    Name:  b y johan 2.de..jpg
Views: 260
Size:  148.0 KB
    Last edited by Oldendum; 01-11-2017 at 05:02 PM.
    "USMCPOP" First-born son: KIA Iraq 1/26/05
    Syncrowave 250 w/ Coolmate 3
    Dialarc 250, Idealarc 250
    SP-175 +
    Firepower TIG 160S (gave the TA 161 STL to the son)
    Lincwelder AC180C (1952)
    Victor & Smith O/A torches
    Miller spot welder

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement