    PowerMax30 Air Error / locked up

    I have 15 minutes on my Powermax30 Air and after ordering parts and metal all week - I begin my project. I get into it for about 5 minutes and notice that when I pull my finger off the trigger, the gun stays powered / still cutting.

    I though my glove was getting stuck in the trigger, so I just kept cutting g down the other side of the angle iron and when I got done - it was pretty clear the gun would not shut off!!

    I pulled the trigger a few times and finally it shut off - but the machine began flashing alternating overtemp and internal compressor. I cycle the power, cycled the trigger, changed voltage - must be a stuck trigger assembly is the only thing I can think of. Is there any other way to reset this thing - it only has a knob and a power switch. Anybody else ever have this issue?

    Too bad because I timed things out not expecting to have a down piece of equipment - especially with 15 minutes on it...

    Thanks in advance is anybody has any recommendations before they open in the morning...

  2. #2
    Join Date
    Jun 2006
    Posts
    26

    Re: PowerMax30 Air Error / locked up

    Solved:

    Trigger switch stuck closed. Disassembled the gun, unplugged the switch and the machine worked fine. Exercised the switch and reassembled - all is good. Prolly need to see if they can send me a new switch.

    Hope this helps somebody else.

  3. #3
    Join Date
    Oct 2007
    Location
    New Hampshire
    Posts
    3,068

    Re: PowerMax30 Air Error / locked up

    Tech Service will take care of you. Have your serial number when you contact them. technical.service@hypertherm.com 0r 1 800 643 9878 . Keep us posted!

    Jim Colt Hypertherm


    Quote Originally Posted by Flywheel View Post
    Solved:

    Trigger switch stuck closed. Disassembled the gun, unplugged the switch and the machine worked fine. Exercised the switch and reassembled - all is good. Prolly need to see if they can send me a new switch.

    Hope this helps somebody else.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement